[论文解读] Calibration and data analysis routines for nanoindentation with spherical tips

Diana Avadanii, Anna Kareer|arXiv (Cornell University)|Feb 5, 2023
Metal and Thin Film MechanicsEngineering参考文献 54被引用 3
一句话总结

本文提出了一种经过验证的、集成化的球形纳米压痕校准与数据分析工作流程,采用弹性参考材料(熔融石英、蓝宝石、非晶碳)独立测定有效压头半径和机器刚度。通过将有效半径参数化为载荷的函数,并将此流程应用于橄榄石、钛和钨等材料,作者提取了精确的压痕应力-应变曲线,并展示了机器刚度对屈服应力识别和压痕尺寸效应评估的决定性影响。

ABSTRACT

Instrumented spherical nanoindentation with a continuous stiffness measurement has gained increased popularity in material science studies in brittle and ductile materials alike. These investigations span hypotheses related to a wide range of microphysics involving grain boundaries, twins, dislocation densities, ion-induced damage and more. These studies rely on the implementation of different methodologies for instrument calibration and for circumventing tip shape imperfections. In this study, we test, integrate, and re-adapt published strategies for tip and machine-stiffness calibration for spherical tips. We propose a routine for independently calibrating the effective tip radius and the machine stiffness using three reference materials (fused silica, sapphire, glassy carbon), which requires the parametrization of the effective radius as a function of load. We validate our proposed workflow against key benchmarks, such as variation of Young's modulus with depth. We apply the resulting calibrations to data collected in materials with varying ductility (olivine, titanium, and tungsten) to extract indentation stress-strain curves. We also test the impact of the machine stiffness on recently proposed methods for identification of yield stress, and compare the influence of different conventions on assessing the indentation size effect. Finally, we synthesize these analysis routines in a single workflow for use in future studies aiming to extract and process data from spherical nanoindentation.

研究动机与目标

  • 解决由压头形状缺陷、机器刚度变化和校准误差引起的球形纳米压痕数据不一致问题。
  • 开发一种统一、可重复的校准流程,仅通过弹性压痕在参考材料上独立测定有效压头半径和机器刚度。
  • 通过深度依赖的杨氏模量和压痕尺寸效应等基准验证该工作流程。
  • 实现从不同延展性材料(如橄榄石、Ti、W)中可靠提取压痕应力-应变曲线。
  • 评估机器刚度对屈服应力识别及分析惯例选择的影响。

提出的方法

  • 使用三种参考材料——熔融石英、蓝宝石和非晶碳——其已知的弹性模量和泊松比用于系统校准。
  • 在低载荷下进行弹性载荷-位移测量,以避免塑性变形,确保赫兹接触力学的有效性。
  • 利用测得的谐振接触刚度和赫兹接触理论,将有效压头半径参数化为施加载荷的函数。
  • 通过将测得的刚度数据拟合至可调节机器柔度的赫兹模型,同时校准机器刚度。
  • 将校准后的参数应用于未知模量材料(橄榄石、Ti、W)的连续刚度测量,以提取压痕应力-应变曲线。
  • 测试机器刚度对屈服应力识别的影响,并比较不同弹出点和尺寸效应分析惯例下的结果。
Figure 1: a) Load-displacement data collected with a spherical tip with a nominal radius of 10 μ m in different materials with known moduli. b) Difference between measured displacements in two materials at similar load. The end cut-off load for each set of experiments is marked by the dashed horizon
Figure 1: a) Load-displacement data collected with a spherical tip with a nominal radius of 10 μ m in different materials with known moduli. b) Difference between measured displacements in two materials at similar load. The end cut-off load for each set of experiments is marked by the dashed horizon

实验结果

研究问题

  • RQ1如何仅通过弹性参考材料的压痕数据,在球形纳米压痕中独立校准有效压头半径和机器刚度?
  • RQ2机器刚度在多大程度上影响球形纳米压痕中屈服应力测定的准确性?
  • RQ3分析惯例的选择如何影响对压痕尺寸效应和弹出行为的解释?
  • RQ4统一的校准工作流程在不同材料和仪器间能否提高压痕应力-应变曲线的一致性和可靠性?
  • RQ5压头形状偏离理想球形的程度对刚度和模量测量有何影响?

主要发现

  • 所提出的校准工作流程能够仅通过参考材料的弹性压痕数据,独立且准确地确定有效压头半径和机器刚度。
  • 有效压头半径被发现随载荷变化,且该依赖关系成功实现参数化,显著优于恒定半径假设的精度。
  • 观察到杨氏模量随深度系统性变化,并得到验证,证实了校准方法的可靠性。
  • 机器刚度显著影响提取的屈服应力,不同校准方法下差异可达15%。
  • 用于识别屈服应力和弹出点的分析惯例选择对报告的压痕尺寸效应有显著影响,凸显了标准化协议的必要性。
  • 该工作流程成功应用于从橄榄石、钛和钨中提取压痕应力-应变曲线,证明了其在不同延展性材料中的实用性。
Figure 2: Summary of results for effective radius determined as the slope of a line fit through data calculated as the subtraction of elastic load-displacement curves at the same load in different reference materials following the method of Li et al. [ 2013 ] (Equation 8 ). The dashed line represent
Figure 2: Summary of results for effective radius determined as the slope of a line fit through data calculated as the subtraction of elastic load-displacement curves at the same load in different reference materials following the method of Li et al. [ 2013 ] (Equation 8 ). The dashed line represent