[论文解读] Effect of PEG binder on gas sensitivity of ferric oxide films synthesized by spin coating and doctor blade methods
本研究探讨了聚乙二醇(PEG)粘合剂对旋涂和刮刀涂覆的三氧化二铁(Fe2O3)薄膜气体传感性能的影响。PEG的引入使气体敏感度提高15.44%,缩短了响应与恢复时间,并降低了光学带隙,主要归因于活化能降低,且未改变主要相结构或官能团,经XRD和FTIR分析确认。
Ferric oxide (Fe2O3) thin films were fabricated on amorphous nonconductive and FTO conductive glass substrates starting from iron acetate nanoparticles by the doctor blade and the spin coating techniques. Thin films of Fe2O3 with and without the PEG binder were investigated. Films were subsequently annealed at 500 0C in air for 1 hour to crystallize the phase Fe2O3. The structural and chemical properties of Fe2O3 thin films were determined using XRD and FTIR. According to XRD, the single phase of Fe2O3 crystallized in the thin film after annealing. The optical band gap of synthesized Fe2O3 thin films were determined by UV-Visible spectrums. Gas sensitivity, respond time and recovery time of Fe2O3 thin films were measured in 1000ppm of CO2 gas using AUTO LAB. Thin films synthesized by the doctor blade method were thicker and more uniform than the thin films prepared by the spin coating technique. Gas sensitivity of Fe2O3 films synthesized by the doctor blade method is slightly higher than that of the films fabricated by the spin coating technique. Fe2O3 films with the PEG binder posses a higher gas sensitivity, lower respond time and lower recovery time compared to films without PEG binder. After adding the PEG binder, the optical band gap of Fe2O3 thin films reduces. The reduction of the activation energy is the reason for the improvement of the gas sensitivity after adding the PEG. However, the peak positions of FTIR do not indicate any significant change due to the adding of the PEG. Adding the binder increased the gas sensitivity of iron oxide by 15.44%. Both FTIR and UV-Visible data confirm the formation of Fe2O3 in the thin film.
研究动机与目标
- 评估PEG粘合剂对旋涂和刮刀涂覆法制备的Fe2O3薄膜气体传感性能的影响。
- 比较含PEG粘合剂与不含PEG粘合剂的Fe2O3薄膜在结构、光学和气体传感性能方面的差异。
- 确定薄膜制备工艺(旋涂与刮刀涂覆)对薄膜形貌和气体敏感度的影响。
- 关联光学带隙与活化能的变化与PEG添加后气体响应增强之间的关系。
- 通过XRD和FTIR光谱学验证纯赤铁矿(α-Fe2O3)相的形成,并评估其化学稳定性。
提出的方法
- 以乙酸铁纳米颗粒为前驱体,制备Fe2O3薄膜。
- 采用旋涂和刮刀涂覆工艺,在FTO玻璃和非导电玻璃基底上沉积薄膜。
- 在空气中以500 °C退火1小时,以获得结晶态α-Fe2O3相。
- 利用X射线衍射(XRD)表征结构特性,通过傅里叶变换红外光谱(FTIR)分析化学组成。
- 采用紫外-可见光谱法测量光学带隙。
- 利用AUTO LAB系统测量1000 ppm CO2下的气体敏感度、响应时间与恢复时间。
实验结果
研究问题
- RQ1PEG粘合剂的添加如何影响旋涂和刮刀涂覆法制备的Fe2O3薄膜的气体敏感度?
- RQ2沉积工艺(旋涂与刮刀涂覆)对薄膜厚度、均匀性及气体传感响应有何影响?
- RQ3PEG的引入如何改变Fe2O3薄膜的光学带隙与活化能?
- RQ4通过FTIR和XRD检测,PEG是否在Fe2O3薄膜中引入了新的官能团或相杂质?
- RQ5PEG添加带来的气体响应、响应时间与恢复时间的定量改善程度如何?
主要发现
- 采用刮刀涂覆法制备的Fe2O3薄膜比旋涂法制备的更厚且更均匀。
- 在Fe2O3薄膜中引入PEG粘合剂后,其气体敏感度提高了15.44%。
- 含PEG的薄膜相比无PEG薄膜表现出更短的响应与恢复时间。
- PEG添加后,Fe2O3薄膜的光学带隙降低,表明其电子电导率得到提升。
- XRD证实退火后形成了单相α-Fe2O3,且PEG的存在未引起衍射峰位置的显著变化。
- FTIR光谱显示PEG未引起显著的化学变化,表明其未改变Fe2O3中的主要化学键合结构。