本研究证明,溅射沉积的ZnO薄膜可增强钴基非晶微线的磁阻抗(MI)响应和场敏感度。通过将ZnO厚度优化至240 nm,MI%从227%提高到406%,场敏感度从1.7%/Oe提升至4.99%/Oe,结构与磁性表征证实ZnO在调控磁导率和MI性能方面发挥了关键作用。
Semiconductive ZnO has shown to be a fascinating element for application in high-performance sensors. ZnO with various thicknesses (87-500 nm) was deposited on the surface of Co-based amorphous micro-wire (Co68.15Fe4.35Si12.5B15) using magnetron sputtering technique and the magnetoimpedance (MI) response was evaluated. The MI% increases monotonously up to the 240 nm thickness of the ZnO layer. By further increase in the ZnO layer thickness the MI% decreases. MI response and field sensitivity increased from 227% and 1.7 %/Oe for bare micro-wire up to 406% and 4.99 %/Oe for ZnO deposited micro-wire with a thickness of 240 nm. The x-ray diffraction (XRD) and scanning electron microscopy (SEM) were used to characterize the structural grown ZnO layers. Vibrating sample magnetometry (VSM) was used to reveal the role of the ZnO thin layer in the MI response. The same trend of increase and decrease in the MI% by thickness was observed for the transverse permeability of the samples determined by VSM. The obtained results address a simple way to achieve high MI response and sensitivity with selective surface sensing.
研究动机与目标
- 研究溅射沉积ZnO薄膜对钴基非晶微线磁阻抗(MI)响应的影响。
- 确定使MI响应和场敏感度最大化的最优ZnO厚度,以适用于传感器应用。
- 通过ZnO包覆理解MI增强背后的结构与磁性机制。
- 探索一种简单、可扩展的表面工程方法,以提升高灵敏度磁传感器的性能。
提出的方法
- 采用磁控溅射法在Co68.15Fe4.35Si12.5B15非晶微线上沉积厚度范围为87至500 nm的ZnO薄膜。
- 通过测量外加磁场下电学阻抗的变化,评估磁阻抗(MI)响应。
- 利用X射线衍射(XRD)和扫描电子显微镜(SEM)表征ZnO薄膜的结构特性。
- 采用振动样品磁强计(VSM)测量横向磁导率,并与MI行为进行关联。
- 系统分析ZnO厚度与MI响应之间的关系,以识别最优厚度。
- 基于零磁场附近MI响应曲线的斜率计算场敏感度。
实验结果
研究问题
- RQ1溅射沉积的ZnO薄膜厚度如何影响钴基微线的磁阻抗响应?
- RQ2何种ZnO厚度可使这些微线的场敏感度和MI百分比达到最大?
- RQ3ZnO薄膜的结构与磁性特性如何与观测到的MI性能相关联?
- RQ4与裸微线相比,ZnO改性在多大程度上增强了横向磁导率和MI响应?
主要发现
- 磁阻抗百分比(MI%)随ZnO厚度增加而单调上升,至240 nm时达到最大值406%。
- 超过240 nm后,进一步增加ZnO厚度导致MI%下降,表明存在性能最优的厚度。
- 场敏感度从裸微线的1.7%/Oe提升至240 nm ZnO厚度时的4.99%/Oe,实现显著增强。
- VSM测得的横向磁导率变化趋势与MI%一致,证实ZnO对响应的磁性贡献。
- XRD与SEM分析证实ZnO薄膜在测试厚度范围内具有良好的结构完整性和均匀性。
- 结果表明,采用ZnO包覆微线的可扩展表面工程方法,可实现高灵敏度磁传感器。