本研究调查了在中子辐照至6×10¹⁵ n/cm²后,滨松光子公司的超快硅探测器(HPK UFSD)的性能表现。这些探测器基于低增益雪崩二极管(LGAD),由于辐射诱导受主移除,其内部增益从约80显著下降至7,时间分辨率从20 ps恶化至50 ps,且在最高辐照剂量下,最优时间分辨率对应的恒 fraction 判定器(CFD)阈值为60%。

ABSTRACT

In this paper we report results from a neutron irradiation campaign of Ultra-Fast Silicon Detectors (UFSD) with fluences of 1e14, 3e14, 6e14, 1e15, 3e15, 6e15 n/cm2. The UFSD used in this study are circular 50 micro-meter thick Low-Gain Avalanche Detectors (LGAD), with a 1.0 mm diameter active area. They have been produced by Hamamatsu Photonics (HPK), Japan, with pre-radiation internal gain in the range 10-100 depending on the bias voltage. The sensors were tested pre-irradiation and post-irradiation with minimum ionizing particle (MIPs) from a 90Sr based \b{eta}-source. The leakage current, internal gain and the timing resolution were measured as a function of bias voltage at -20C and -30C. The timing resolution was extracted from the time difference with a second calibrated UFSD in coincidence, using the constant fraction method for both. The dependence of the gain upon the irradiation fluence is consistent with the concept of acceptor removal and the gain decreases from about 80 pre-irradiation to 7 after a fluence of 6e15 n/cm2. Consequently, the timing resolution was found to deteriorate from 20 ps to 50 ps. The results indicate that the most accurate time resolution is obtained at a value of the constant fraction discriminator (CFD) threshold used to determine the time of arrival varying with fluence, from 10% pre-radiation to 60% at the highest fluence. Key changes to the pulse shape induced by irradiation, i.e. (i) a reduce sensitivity of the pulse shape on the initial non-uniform charge deposition, (ii) the shortening of the rise time and (iii) the reduced pulse height, were compared with the WF2 simulation program and found to be in agreement.

研究动机与目标

  • 评估HPK UFSD在中子注量达6×10¹⁵ n/cm²下的辐射耐受性。
  • 理解中子辐照对关键探测器参数(漏电流、内部增益和时间分辨率)的影响。
  • 确定辐照后用于飞行时间测量的最优恒 fraction 判定器(CFD)阈值。
  • 通过WF2模拟程序将观测到的脉冲波形变化与辐射诱导缺陷相关联。

提出的方法

  • 在1×10¹⁴、3×10¹⁴、6×10¹⁴、1×10¹⁵、3×10¹⁵和6×10¹⁵ n/cm²的注量下进行中子辐照。
  • 使用⁹⁰Sr β源在辐照前后对UFSD进行测量,以暴露于最小电离粒子(MIPs)。
  • 在-20°C和-30°C下,测量漏电流、内部增益和时间分辨率随偏置电压的变化。
  • 通过与经过校准的参考UFSD在符合模式下使用恒 fraction 方法提取时间分辨率。
  • 分析并比较脉冲波形变化与使用WF2程序模拟辐射诱导缺陷的结果。
  • 系统研究了在所有注量水平下,时间分辨率对CFD阈值的依赖性。

实验结果

研究问题

  • RQ1中子辐照如何影响HPK UFSD在高达6×10¹⁵ n/cm²注量下的内部增益?
  • RQ2随着中子注量的增加,时间分辨率如何演变,其对CFD阈值设置的依赖性如何?
  • RQ3辐射诱导缺陷如何改变脉冲波形特性,如上升时间、脉冲幅度以及对初始电荷沉积非均匀性的敏感性?
  • RQ4观测到的脉冲波形变化在多大程度上与WF2程序的预测一致?
  • RQ5在每个辐照注量水平下,实现最佳时间分辨率的最优CFD阈值设置是什么?

主要发现

  • HPK UFSD的内部增益在辐照前约为80,辐照至6×10¹⁵ n/cm²后下降至7。
  • 时间分辨率从辐照前的20 ps恶化至最高注量6×10¹⁵ n/cm²下的50 ps。
  • 为实现最佳时间分辨率,CFD阈值从低注量下的10%移至6×10¹⁵ n/cm²下的60%。
  • 辐照导致脉冲上升时间缩短,脉冲幅度降低,对初始电荷非均匀性的敏感性下降。
  • 观测到的脉冲波形变化与WF2程序的模拟结果高度一致。
  • 增益退化与受主移除模型一致,表明LGAD结构中形成了辐射诱导缺陷。