本研究利用相干反射计测量硅在毫米波波段的损耗 tangent,通过分析介质板中的法布里-珀罗干涉条纹,得出中子辐照硅的损耗 tangent 为 2.8×10⁻⁴,本征硅的损耗 tangent 为 1.5×10⁻⁵,两者折射率均为 3.41,证明硅在毫米波接收机中作为低损耗温态光学元件的可行性。
We report here on measurements of the reflectivity and loss tangent measured in the W-band (80-125 GHz) and D-band (125-180 GHz) in two samples of float zone silicon with intrinsic stoichiometry - one irradiated by neutrons, which increases the resistivity by introducing crystalline defects, and the other unperturbed. We find a loss tangent $ an(δ)$ of 2.8e-4 and 1.5e-5 for neutron-irradiated silicon and intrinsic silicon, respectively, both with an index of refraction of 3.41. The results demonstrate the applicability of silicon as a warm optical component in millimeter-wave receivers. For our measurements, we use a coherent reflectometer to measure the Fabry-Perot interference fringes of the reflected signal from dielectric slabs. The depth of the reflection nulls provides a sensitive measurement of dielectric losses. We describe the test setup which can also characterize scattering and transmission, and can provide detailed characterization of millimeter wave materials.
研究动机与目标
- 测量适用于天体物理学仪器的毫米波段硅的介电损耗。
- 评估中子辐照对硅损耗 tangent 及光学性能的影响。
- 证明硅可作为毫米波接收机中温态光学元件的应用可行性。
- 验证基于反射计的测量方法在 W 波段和 D 波段表征介电材料的准确性。
提出的方法
- 相干反射计测量介质板反射信号的幅度和相位。
- 通过分析反射信号中的法布里-珀罗干涉条纹提取介电损耗。
- 利用反射谷深作为介电损耗的灵敏指示参数。
- 该装置可实现对毫米波材料反射、透射和散射特性的表征。
- 测量在 W 波段(80–125 GHz)和 D 波段(125–180 GHz)范围内进行。
- 假设并采用折射率为 3.41,用于解释损耗 tangent 值。
实验结果
研究问题
- RQ1本征浮区硅在毫米波段的损耗 tangent 是多少?
- RQ2中子辐照如何影响硅在 80–180 GHz 频率范围内的损耗 tangent?
- RQ3硅能否作为毫米波接收机中低损耗温态光学元件?
- RQ4在反射计装置中,利用法布里-珀罗条纹分析测量介电损耗的精度如何?
主要发现
- 中子辐照硅在 W 波段和 D 波段的损耗 tangent 测量值为 2.8×10⁻⁴。
- 本征浮区硅在同一频段范围内的损耗 tangent 测量值为 1.5×10⁻⁵。
- 两种硅样品的折射率均为 3.41,测量结果一致。
- 反射计装置通过谷深分析可灵敏检测介电损耗。
- 结果证实硅是毫米波接收机中温态光学元件的合适材料。
阅读本论文
在 Nubint 阅读器中打开原文,边读边就任意段落提问。
在 Nubint 中阅读本论文本解读由 AI 根据论文原文生成,引用前请核对原文。