Skip to main content
QUICK REVIEW

[论文解读] Structural phase transition, grain growth and optical properties of uncompensated Ga-V co-doped TiO2

Nasima Khatun, Saurabh Tiwari|arXiv (Cornell University)|Jun 24, 2018
Chalcogenide Semiconductor Thin FilmsEngineering被引用 4
一句话总结

本研究探究了未补偿掺杂的Ga-V共掺杂TiO2,结果表明,共掺杂通过将相变活化能从120 kJ/mol提高至140 kJ/mol,使金红石相在约650 °C以下保持稳定。共掺杂显著提升了比表面积(最高达96.53 m²/g),将带隙缩小至可见光范围,并促进金红石相颗粒呈棒状生长,使该材料在高温下对可见光光催化具有高度有效性。

ABSTRACT

Effect of uncompensated Ga-V co-doping on structural phase transition, grain growth process and optical properties of TiO2 is reported here. Inhibition of phase transition due to co-doping is confirmed by X-ray diffraction measurement. Activation energy of phase transition increases from 120KJ/mol (x=0) to 140 KJ/mol (x=0.046) due to Ga-V co-doping. In anatase phase, lattice constants increase by the effect of Ga3+ interstitials. This results in inhibition of phase transition. Anatase phase becomes stable up to ~650 C in co-doped sample whereas for pure TiO2 phase transition starts in between 450-500 C. In anatase phase, strain increases due to co-doping which reduces crystallite size. In rutile phase, grain growth process is enhanced due to co-doping and particles show a rod-like structure with majority 110 facets. Bandgap decreases in both phases and reduced to a visible light region. BET analysis shows that surface area increases from 4.55 m2/g (x=0) to 96.53 m2/g (x=0.046) by Ga-V incorporation which provide a large number of active site for photocatalytic activity. Hence, co-doped anatase nanoparticle can be used as a promising candidate for photocatalytic applications using visible light up to a higher temperature ~650 C.

研究动机与目标

  • 探究未补偿Ga-V共掺杂对TiO2结构与光学性能的影响。
  • 理解共掺杂如何影响TiO2的相变动力学与晶粒生长行为。
  • 评估通过增加比表面积和带隙窄化对光催化活性的提升效果。
  • 确定共掺杂TiO2中金红石相的热稳定性极限,以适用于高温应用。

提出的方法

  • 采用X射线衍射(XRD)分析Ga-V共掺杂TiO2中的相变行为及晶格常数变化。
  • 通过XRD数据的Rietveld精修定量测定金红石相的晶格常数与应变。
  • 采用BET比表面积分析测定共掺杂引起的比表面积变化。
  • 通过紫外-可见漫反射光谱测定带隙能。
  • 利用热分析数据,结合阿伦尼乌斯方程计算相变活化能。
  • 通过电子显微镜分析揭示金红石相中晶粒生长与晶面发育情况。

实验结果

研究问题

  • RQ1Ga-V共掺杂如何影响TiO2的相变温度?
  • RQ2Ga3+间隙离子对金红石相的晶格常数与应变有何影响?
  • RQ3共掺杂如何影响金红石相的晶粒生长与形貌特征?
  • RQ4共掺杂在多大程度上降低了带隙并提升了比表面积,以增强光催化性能?
  • RQ5Ga-V共掺杂TiO2中金红石相的热稳定性极限是多少?

主要发现

  • 在纯TiO2中,相变活化能为120 kJ/mol,而在Ga-V共掺杂TiO2(x=0.046)中提升至140 kJ/mol。
  • 在共掺杂样品中,金红石相在约650 °C以下保持稳定,而纯TiO2中仅能稳定至450–500 °C。
  • 由于Ga3+间隙离子的引入,金红石相的晶格常数增大,有助于相的稳定。
  • 比表面积从纯TiO2的4.55 m²/g显著提升至共掺杂样品(x=0.046)的96.53 m²/g。
  • 在金红石相与金红石相中,带隙均被缩小至可见光区域,增强了对可见光的吸收。
  • 金红石相颗粒表现出棒状形貌,且主要晶面为(110),这是由于共掺杂促进了晶粒生长。

阅读本论文

在 Nubint 阅读器中打开原文,边读边就任意段落提问。

在 Nubint 中阅读本论文

本解读由 AI 根据论文原文生成,引用前请核对原文。