[论文解读] The perovskite/transport layer interfaces dominate non-radiative recombination in efficient perovskite solar cells
本研究量化在多种 CTL 下的钙钛矿/传输层界面的非辐射性界面复合,结果表明这些界面主要限制 V_OC,并且这些界面的选择性对接近辐射极限至关重要。
Charge transport layers (CTLs) are key components of diffusion controlled perovskite solar cells, however, they can induce additional non-radiative recombination pathways which limit the open circuit voltage (V_OC) of the cell. In order to realize the full thermodynamic potential of the perovskite absorber, both the electron and hole transport layer (ETL/HTL) need to be as selective as possible. By measuring the quasi-Fermi level splitting (QFLS) of perovskite/CTL heterojunctions, we quantify the non-radiative interfacial recombination current for a wide range of commonly used CTLs, including various hole-transporting polymers, spiro-OMeTAD, metal oxides and fullerenes. We find that all studied CTLs limit the V_OC by inducing an additional non-radiative recombination current that is significantly larger than the loss in the neat perovskite and that the least-selective interface sets the upper limit for the V_OC of the device. The results also show that the V_OC equals the internal QFLS in the absorber layer of (pin, nip) cells with selective CTLs and power conversion efficiencies of up to 21.4%. However, in case of less selective CTLs, the V_OC is substantially lower than the QFLS which indicates additional losses at the contacts and/or interfaces. The findings are corroborated by rigorous device simulations which outline several important considerations to maximize the V_OC. This work shows that the real challenge to supress non-radiative recombination losses in perovskite cells on their way to the radiative limit lies in the suppression of carrier recombination at the perovskite/CTL interfaces.
研究动机与目标
- 评估不同电荷传输层(CTLs)如何影响钙钛矿界面的非辐射重组。
- 通过准费米能级分裂(QFLS)测量来量化界面非辐射电流。
- 确定CTL选择性如何相对于吸收体的QFLS支配开路电压(V_OC)。
- 为优化CTL选择以接近钙钛矿电池的辐射极限提供指导。
提出的方法
- 测量钙钛矿/CTL异质结的准费米能级分裂(QFLS),以量化非辐射界面重组电流。
- 测试包括空穴传输聚合物、spiro-OMeTAD、金属氧化物和富勒烯在内的广泛CTL。
- 在具有选择性 vs 非选择性 CTL 的器件中,将 V_OC 与吸收体 QFLS 进行比较。
- 使用器件仿真来解释界面重组如何影响 V_OC,并指导优化。
实验结果
研究问题
- RQ1不同的钙钛矿/CTL界面引起的非辐射重组有多大?
- RQ2CTL选择性在多大程度上限制了开路电压相对于吸收体内部 QFLS?
- RQ3选择性 CTLs 是否能使 V_OC 与吸收体的 QFLS 匹配并接近辐射极限?
- RQ4仿真给出哪些通过抑制界面重组来最大化 V_OC 的指导?
- RQ5是否存在与降低非辐射界面损失相关的可识别 CTL 特性?
主要发现
- 所有研究的 CTL 都会引入额外的非辐射性界面重组,超过单独钙钛矿的损失。
- 最不具选择性的界面设定了器件 V_OC 的上限。
- 当 CTLs 具有选择性时,(pin, nip) 电池的 V_OC 等于吸收体的内部 QFLS,效率高达 21.4%。
- 使用较少选择性的 CTLs 时,V_OC 明显低于 QFLS,表明存在接触/界面额外损失。
- 严谨的器件仿真证实,最大化 V_OC 需要抑制钙钛矿/CTL 界面的复合。
阅读本论文
在 Nubint 阅读器中打开原文,边读边就任意段落提问。
在 Nubint 中阅读本论文本解读由 AI 根据论文原文生成,引用前请核对原文。