[Paper Review] An integrated DEM-FEM approach to study breakage in packing of glass cartridges on a conveyor belt
This study presents an integrated DEM-FEM approach to simulate stress accumulation and crack initiation in glass cartridges during conveyor belt transport in pharmaceutical packaging. By modeling cartridges as equivalent spheres in DEM to capture collision dynamics, and applying FEM to compute time-varying principal stresses, the study identifies localized tensile stress peaks up to 140 MPa at contact zones, with critical crack initiation likely from the inner wall due to compressive-tensile stress gradients.
The use of glass for pharmaceutical new applications such as high-technology drugs, requires the strictest container inertness. A common theme of paramount importance in glass container integrity preservation is the detailed mechanism driving the sudden failure due the crack propagation. Using a combination of Discrete Element Method (DEM) and Finite Element Method (FEM), a stress map for glass cartridges packed into an accumulation table and transported by a conveyor belt at a fixed velocity is obtained under realistic conditions. The DEM calculation provides a full description of the dynamics of the cartridges, as approximated by an equivalent sphere, as well as the statistics of the multiple collisions. The FEM calculation exploits this input to provide the maximum principal stress of different pairs as a function of time. Our analysis shows that, during their transportation on the conveyor belt, the cartridges are subject to several shocks of varying intensities. Under these conditions, a crack may originate inside the cartridge in the area of maximal tensile stress, and propagate outward. Estimated stresses are found in good agreement with real systems.
Motivation & Objective
- To investigate the mechanical failure mechanisms of glass cartridges during high-density packing and transport on a conveyor belt.
- To identify the conditions under which micro-cracks initiate and propagate due to dynamic impacts in a packed system.
- To develop a computationally feasible simulation framework combining DEM and FEM for predicting stress distribution in brittle glass containers.
- To assess the risk of sudden cartridge breakage due to localized tensile stresses from multiple collisions.
- To provide a predictive model for industrial risk assessment in pharmaceutical primary packaging.
Proposed method
- Discrete Element Method (DEM) using the Yade package to simulate the dynamics of equivalent spherical particles representing glass cartridges under high packing density.
- Each cartridge is modeled as 632 small spheres to preserve geometric fidelity while reducing computational cost.
- DEM tracks collision frequency, contact forces, relative velocities, and contact positions over time.
- Finite Element Method (FEM) uses DEM-derived contact forces and kinematics as input to compute the full stress tensor field in the glass wall.
- The FEM model computes maximum principal stress over time, with emphasis on stress gradients through the glass thickness.
- Non-linear and no-tension spring models are used to simulate different contact behaviors and their effects on stress concentration.
Experimental results
Research questions
- RQ1What are the dominant collision dynamics and force distributions in a packed system of glass cartridges on a conveyor belt?
- RQ2Where and when do peak tensile stresses occur in the glass wall during dynamic impacts?
- RQ3How does the stress distribution through the glass thickness correlate with crack initiation potential?
- RQ4What role do contact force intensity and direction play in inducing critical stress levels?
- RQ5Can an equivalent sphere model accurately represent the mechanical response of real cylindrical glass cartridges under impact?
Key findings
- Peak maximum principal stress reaches 140 MPa at the bottom of cartridge 1 during impact with pair 1-3 under no-tension spring conditions.
- The maximum principal tensile stress of 94 MPa occurs inside the cartridge wall at the contact zone for pair 1-3 with no-tension springs, indicating high crack initiation risk.
- Stress distribution shows a shifting trend from compression on the outer surface to tension on the inner surface at the impact zone, favoring crack nucleation from the inside.
- Crack propagation is predicted to initiate internally and propagate outward, a dangerous scenario leading to sudden rupture and production line stoppages.
- The stress field evolution is highly sensitive to contact force history, with significant fluctuations due to chaotic dynamics in high-density packing.
- The model shows good agreement with real-world stress levels observed in industrial systems, validating the DEM-FEM integration approach.