[Paper Review] Angular harmonic Hall voltage and magnetoresistance measurements of Pt/FeCoB and Pt-Ti/FeCoB bilayers for spin Hall conductivity determination
This paper presents a comprehensive experimental protocol for accurately determining spin Hall conductivity (σSH) in Pt/FeCoB and Pt-Ti/FeCoB bilayers using angular harmonic Hall voltage and ferromagnetic resonance measurements. By combining low-noise static transport, dynamic FMR, and interface transparency corrections, the authors achieve a record σSH of 3.3×10⁵ S/m in 5.6 nm Pt, exceeding values in W, Ta, and other heavy metals, establishing Pt as a top-tier material for spintronic applications.
Materials with significant spin-orbit coupling enable efficient spin-to-charge interconversion, which can be utilized in novel spin electronic devices. A number of elements, mainly heavy-metals (HM) have been identified to produce a sizable spin current ($j_\mathrm{s}$), while supplied with a charge current ($j$), detected mainly in the neighbouring ferromagnetic (FM) layer. Apart from the spin Hall angle $ heta_\mathrm{SH}$ = $j_\mathrm{s}$/$j$, spin Hall conductivity ($\sigma_\mathrm{SH}$) is an important parameter, which takes also the resistivity of the material into account. In this work, we present a measurement protocol of the HM/FM bilayers, which enables for a precise $\sigma_\mathrm{SH}$ determination. Static transport measurements, including resistivity and magnetization measurements are accompanied by the angular harmonic Hall voltage analysis in a dedicated low-noise rotating probe station. Dynamic characterization includes effective magnetization and magnetization damping measurement, which enable HM/FM interface absorption calculation. We validate the measurement protocol in Pt and Pt-Ti underlayers in contact with FeCoB and present the $\sigma_\mathrm{SH}$ of up to 3.3$ imes$10$^5$ S/m, which exceeds the values typically measured in other HM, such as W or Ta.
Motivation & Objective
- To develop a robust, multi-frequency measurement protocol for precise spin Hall conductivity (σSH) determination in HM/FM bilayers.
- To overcome limitations of existing methods by avoiding strict requirements like perpendicular magnetic anisotropy or negligible field-like torque.
- To validate the protocol on Pt/FeCoB and Pt-Ti/FeCoB systems, enabling accurate extraction of σSH, θSH, and interface transparency.
- To quantify the impact of Pt thickness and Pt-Ti interface number on spin transport properties, including resistivity and damping.
- To establish Pt and Pt-Ti/FeCoB as high-performance candidates for spin-orbit torque devices by benchmarking σSH against other materials.
Proposed method
- Employed a low-noise, rotating probe station with a linear driver to enable ultra-sensitive nV-resolution measurements of harmonic Hall voltages.
- Conducted angular-dependent Hall voltage and magnetoresistance measurements in x-y (α), y-z (β), and x-z (γ) planes to separate AMR and SMR contributions.
- Used ferromagnetic resonance (FMR) to extract effective magnetization, damping, and spin absorption at the HM/FM interface.
- Applied a model-based analysis combining resistivity, magnetization, and FMR data to calculate spin Hall conductivity σSH = ξSH / ρHM.
- Incorporated interface transparency (T) into the intrinsic spin Hall angle calculation: θSH = ξDL / T, with T derived from spin diffusion length and mixing conductance.
- Fabricated Hall-bar devices via two-step lithography and ion-beam etching on Pt-wedge and Pt-Ti multilayer stacks for systematic thickness and interface variation.
Experimental results
Research questions
- RQ1Can a unified measurement protocol accurately determine spin Hall conductivity (σSH) in Pt/FeCoB and Pt-Ti/FeCoB bilayers without requiring specialized magnetic anisotropy?
- RQ2How does the spin Hall conductivity (σSH) vary with Pt thickness and the number of Pt-Ti interfaces in multilayer structures?
- RQ3What is the role of interface transparency in determining the intrinsic spin Hall angle (θSH), and how does it affect σSH calculations?
- RQ4How do the measured SMR and AMR contributions correlate with σSH and resistivity across different bilayer configurations?
- RQ5Can Pt-based systems achieve higher σSH than other heavy metals like W or Ta, and what factors enable this performance?
Key findings
- The spin Hall conductivity (σSH) in 5.6 nm thick Pt/FeCoB reaches 3.3×10⁵ S/m, among the highest values reported for any heavy metal or alloy.
- For Pt-Ti/FeCoB, σSH reaches 3.2×10⁵ S/m with 3 Pt-Ti interfaces, demonstrating that interface engineering enhances σSH without sacrificing conductivity.
- The intrinsic spin Hall angle (θSH) reaches 0.35 for 5.6 nm Pt, with values ranging from 0.12 to 0.35 depending on Pt thickness and interface structure.
- Spin Hall magnetoresistance (SMR) scales with σSH across all samples, while resistivity shows an inverse trend, confirming σSH as a key figure of merit.
- Interface transparency (T) ranges from 0.42 to 0.51, and correcting for T significantly increases the intrinsic θSH, with values up to 0.35 for Pt.
- The protocol successfully decouples AMR and SMR contributions, enabling accurate extraction of spin transport parameters even in polycrystalline, non-perpendicularly anisotropic systems.
Read this paper
Open the full text in the Nubint reader and ask about any passage as you read.
Read this paper on NubintThis review was generated by AI from the original paper. Please check the paper before citing it.