[Paper Review] Autonomous Repair in Cementitous Material by Combination of Superabsorbent Polymers and Polypropylene Fibres: A Step Towards Sustainable Infrastructure
This study proposes a self-healing cementitious composite combining polypropylene (PP) fibers and superabsorbent polymers (SAP) to autonomously seal cracks and restore mechanical and durability properties. The system achieves up to 90% recovery of durability and full mechanical strength recovery after healing, with 85% crack-sealing efficiency under moist conditions and complete sealing of cracks up to 330 µm via carbonate precipitation.
Manual maintenance and repair of cracks in concrete structures are often unsustainable because of associated labor, capital and environmental damage. Introduction of microfibers and superabsorbent polymers is a material solution to restrict crack propagation and enhance self-healing efficiency. Therefore, the study proposes a combination of polypropylene(PP) fibers and superabsorbent polymers (SAP) which would facilitate autonomous healing and recover original mechanical and durability properties of mortar. Mechanical strength, sorptivity and water penetration of healed mortars were compared to that of undamaged mortar at same age to estimate recovery of original properties while crack sealing was investigated by means of optical microscopy. Experimental results show mortar with combination of PP fibers and SAP showed full recovery of mechanical strength after healing while recovery in durability up to 90% was recorded. Microscopic images show that average crack-sealing ratio of 85% could be achieved under moist condition by combination of SAP and PP fibers while sealing under drier air curing condition is also significantly higher than reference samples with only fibers. Crack width up to 330μm has been found to be completely sealed by carbonate crystals. Furthermore, mortar with SAP and PP fibers retain about 70% of their original 28-day strength after three cycles of loading while reference mortar samples were found to retain only about 40-50% of their original strength. Effective crack sealing and high recovery of original properties in mortars with SAP and fibers suggest that this material combination would reduce the need for environmentally damaging and expensive repairs during the service life.
Motivation & Objective
- To address the unsustainable costs and environmental impact of manual repair in concrete infrastructure.
- To develop a self-healing cementitious material that autonomously seals cracks without external intervention.
- To enhance both mechanical strength and durability recovery in cracked mortar through a synergistic combination of PP fibers and SAP.
- To evaluate the effectiveness of the hybrid system under varying environmental conditions (moist vs. dry curing).
Proposed method
- Incorporated polypropylene (PP) fibers and superabsorbent polymers (SAP) into mortar mixtures at controlled dosages.
- Used optical microscopy to analyze crack sealing efficiency and morphology of healed regions.
- Conducted mechanical testing (compressive strength) on specimens before and after multiple loading cycles to assess strength recovery.
- Measured sorptivity and water penetration to evaluate durability recovery post-healing.
- Cured specimens under both moist and dry conditions to assess environmental influence on healing performance.
- Monitored formation of carbonate crystals in healed cracks via microscopy and chemical analysis.
Experimental results
Research questions
- RQ1Can the combination of PP fibers and SAP enable autonomous crack healing in cementitious materials?
- RQ2To what extent can mechanical strength and durability be recovered in cracked mortar after self-healing?
- RQ3How does environmental humidity (moist vs. dry curing) affect the crack-sealing efficiency of the hybrid system?
- RQ4What is the maximum crack width that can be fully sealed by the self-healing mechanism?
- RQ5How does the hybrid system compare to fiber-only or SAP-only systems in terms of strength retention after cyclic loading?
Key findings
- Mortar with PP fibers and SAP achieved full recovery of mechanical strength after healing, compared to undamaged control specimens.
- Durability recovery reached up to 90% as measured by sorptivity and water penetration tests.
- An average crack-sealing ratio of 85% was achieved under moist curing conditions.
- Crack widths up to 330 µm were completely sealed by carbonate crystals formed during the healing process.
- After three loading cycles, the hybrid mortar retained approximately 70% of its original 28-day strength, significantly outperforming reference samples that retained only 40–50%.
- Crack sealing under dry curing conditions was still significantly higher than in reference samples with only PP fibers, indicating enhanced healing potential in variable environments.
Read this paper
Open the full text in the Nubint reader and ask about any passage as you read.
Read this paper on NubintThis review was generated by AI from the original paper. Please check the paper before citing it.