[Paper Review] Fabrication and in vitro characterization of three-dimensional organic/inorganic scaffolds by robocasting

J. Russias, Eduardo Saiz|arXiv (Cornell University)|Mar 28, 2018
Bone Tissue Engineering MaterialsEngineering31 references6 citations
TL;DR

This study demonstrates the room-temperature robocasting of 3D hybrid organic/inorganic scaffolds using polylactide or polycaprolactone matrices with hydroxyapatite (up to 70 wt%) or bioactive glass, achieving controlled pore sizes (200–500 µm). The scaffolds exhibit anisotropic mechanical behavior, high stiffness with minimal brittleness, and maintain structural integrity in simulated body fluid, with bioactive glass scaffolds forming an apatite layer after 20 days.

ABSTRACT

A key issue for the fabrication of scaffolds for tissue engineering is the development of processing techniques flexible enough to produce materials with a wide spectrum of solubility (bioresorption rates) and mechanical properties matching those of calcified tissues. These techniques must also have the capability of generating adequate porosity to further serve as a framework for cell penetration, new bone formation, and subsequent remodeling. In this study, we show how hybrid organic/inorganic scaffolds with controlled microstructures can be built using robotic assisted deposition at room temperature. Polylactide or polycaprolactone scaffolds with pore sizes ranging between 200-500 μm and hydroxyapatite contents up to 70 wt % were fabricated. Compressive tests revealed an anisotropic behavior of the scaffolds, strongly dependent on their chemical composition. The inclusion of an inorganic component increased their stiffness but they were not brittle and could be easily machined even for ceramic contents up to 70 wt%. The mechanical properties of hybrid scaffolds did not degrade significantly after 20 days in simulated body fluid. However, the stiffness of pure polylactide scaffolds increased drastically due to polymer densification. Scaffolds containing bioactive glasses were also printed. After 20 days in simulated body fluid they developed an apatite layer on their surface.

Motivation & Objective

  • To develop a flexible fabrication technique for tissue engineering scaffolds with variable bioresorption rates and mechanical properties matching calcified tissues.
  • To address the challenge of creating scaffolds with adequate porosity for cell infiltration and new bone formation.
  • To produce hybrid scaffolds with controlled microstructures using room-temperature robotic deposition.
  • To evaluate the mechanical stability and bioactivity of scaffolds in simulated physiological conditions.
  • To investigate the influence of inorganic content (hydroxyapatite, bioactive glass) on scaffold performance and degradation behavior.

Proposed method

  • Robotic deposition (robocasting) was used to fabricate 3D scaffolds at room temperature, enabling precise control over geometry and porosity.
  • Polylactide (PLA) or polycaprolactone (PCL) were used as organic matrices with hydroxyapatite (up to 70 wt%) or bioactive glass as inorganic components.
  • Pore sizes were systematically controlled between 200–500 µm to support cell penetration and tissue ingrowth.
  • Mechanical characterization via compressive testing assessed anisotropy and stiffness as functions of composition and ceramic content.
  • In vitro testing in simulated body fluid (SBF) for 20 days evaluated structural stability, surface reactivity, and apatite formation.
  • Surface analysis techniques confirmed apatite layer development on bioactive glass-containing scaffolds after SBF exposure.

Experimental results

Research questions

  • RQ1Can robocasting produce 3D hybrid scaffolds with tunable porosity and controlled microstructure at room temperature?
  • RQ2How does the inclusion of hydroxyapatite or bioactive glass affect the mechanical properties and anisotropy of organic/inorganic scaffolds?
  • RQ3What is the mechanical stability of hybrid scaffolds after prolonged exposure to simulated body fluid?
  • RQ4Does the incorporation of bioactive glass induce apatite layer formation on the scaffold surface in SBF?
  • RQ5How does the mechanical behavior of pure polylactide scaffolds change after immersion in SBF due to polymer densification?

Key findings

  • Robocasting enabled the fabrication of 3D scaffolds with pore sizes ranging from 200 to 500 µm and hydroxyapatite contents up to 70 wt%.
  • Compressive testing revealed anisotropic mechanical behavior, with stiffness increasing significantly with inorganic content, yet the scaffolds remained non-brittle and machinable.
  • Scaffolds with 70 wt% hydroxyapatite maintained mechanical integrity after 20 days in simulated body fluid, showing no significant degradation.
  • Pure polylactide scaffolds exhibited a drastic increase in stiffness after 20 days in SBF due to polymer densification.
  • Bioactive glass-containing scaffolds developed a surface apatite layer after 20 days in SBF, indicating strong bioactivity.
  • The mechanical properties of hybrid scaffolds were not significantly compromised after 20 days in SBF, confirming their stability for long-term tissue engineering applications.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.