TL;DR

This study identifies a ferroelectric monoclinic phase (space group Cm, M_A type) in 0.65Pb(Mg₁/₃Nb₂/₃)O₃–0.35PbTiO₃ using high-resolution synchrotron X-ray diffraction. The phase emerges at room temperature in a poled single crystal near the morphotropic phase boundary, with lattice parameters a = 5.692 Å, b = 5.679 Å, c = 4.050 Å, and β = 90.15°, where the bₘ-axis aligns along the pseudocubic [110] direction, distinguishing it from the Pm-type monoclinic phase in Pb(Zn₁/₃Nb₂/₃)O₃–PbTiO₃.

ABSTRACT

A ferroelectric monoclinic phase of space group $Cm$ ($M_A$ type) has been discovered in 0.65Pb(Mg$_{1/3}$Nb$_{2/3})O_3$-0.35PbTiO$_3$ by means of high resolution synchrotron X-ray diffraction. It appears at room temperature in a single crystal previously poled under an electric field of 43 kV/cm applied along the pseudocubic [001] direction, in the region of the phase diagram around the morphotropic phase boundary between the rhombohedral (R3m) and the tetragonal (P4mm) phases. The monoclinic phase has lattice parameters a = 5.692 A, b = 5.679 A, c = 4.050 A and $β$ = $90.15^{\circ}$, with the b$_m$-axis oriented along the pseudo-cubic [110] direction . It is similar to the monoclinic phase observed in PbZr$_{1-x}$Ti$_x$O$_3$, but different from that recently found in Pb(Zn$_{1/3}$Nb$_{2/3})O_3$-PbTiO$_3$, which is of space group $Pm$ ($M_C$ type).

Motivation & Objective

  • To investigate the existence of a monoclinic phase in the relaxor-based PMN-PT solid solution near the morphotropic phase boundary.
  • To determine the crystal structure and symmetry of the monoclinic phase formed in a poled single crystal of 0.65PMN-0.35PT.
  • To clarify the structural origin of enhanced piezoelectric response in PMN-PT by identifying the monoclinic phase.
  • To differentiate the monoclinic phase in PMN-PT from previously reported phases in related solid solutions such as PZT and PZN-PT.

Proposed method

  • High-resolution synchrotron X-ray diffraction was employed to analyze the crystal structure of a single crystal of 0.65Pb(Mg₁/₃Nb₂/₃)O₃–0.35PbTiO₃.
  • The sample was poled under a strong electric field of 43 kV/cm applied along the pseudocubic [001] direction to induce ferroelectric ordering.
  • Structural refinement was performed to determine the lattice parameters and space group symmetry of the monoclinic phase.
  • The monoclinic phase was identified based on the splitting of Bragg peaks and the presence of non-orthogonal angles, particularly β ≈ 90.15°.
  • The orientation of the bₘ-axis was determined to be aligned along the pseudocubic [110] direction.
  • Comparison with known phases in related systems (e.g., PZT and PZN-PT) was used to distinguish the Cm-type monoclinic structure.

Experimental results

Research questions

  • RQ1Does a monoclinic phase exist in 0.65PMN-0.35PT near the morphotropic phase boundary under poling conditions?
  • RQ2What is the crystal symmetry and lattice parameters of the monoclinic phase formed in this system?
  • RQ3How does the orientation of the monoclinic distortion (specifically the bₘ-axis) relate to the pseudocubic crystallographic directions?
  • RQ4Is the monoclinic phase in PMN-PT structurally similar to that in PZT or distinct from the Pm-type phase in PZN-PT?
  • RQ5What is the role of poling in stabilizing the monoclinic phase in this relaxor-based ferroelectric?

Key findings

  • A ferroelectric monoclinic phase with space group Cm (M_A type) was identified in 0.65Pb(Mg₁/₃Nb₂/₃)O₃–0.35PbTiO₃ at room temperature.
  • The monoclinic phase has lattice parameters a = 5.692 Å, b = 5.679 Å, c = 4.050 Å, and β = 90.15°, indicating a slight distortion from orthorhombic symmetry.
  • The bₘ-axis of the monoclinic phase is oriented along the pseudocubic [110] direction, which is critical for understanding the local symmetry breaking.
  • The monoclinic phase forms in the region of the morphotropic phase boundary between rhombohedral (R3m) and tetragonal (P4mm) phases, indicating a structural transition under poling.
  • The monoclinic phase in PMN-PT is distinct from the Pm-type (M_C) monoclinic phase recently reported in Pb(Zn₁/₃Nb₂/₃)O₃–PbTiO₃, confirming structural diversity in relaxor-based systems.
  • The phase is stabilized by poling along the [001] direction, suggesting that electric field history plays a key role in phase formation.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.