Skip to main content
QUICK REVIEW

[Paper Review] Nematic properties of FeSe$_{1-x}$Te$_{x}$ crystals with a low Te content

E. A. Ovchenkov, Д. А. Чареев|arXiv (Cornell University)|Sep 2, 2019
Iron-based superconductors researchMaterials Science29 references6 citations
TL;DR

This study investigates nematic properties in low-Te-doped FeSe1-xTex single crystals (x = 0.17, 0.21, 0.25), synthesizing high-quality samples via a flux method at elevated temperatures to stabilize solid solutions. Transport measurements reveal a nematic transition at ~70–60 K, a hole-to-electron carrier type inversion above x = 0.17, and a sign reversal in elastoresistivity from positive to negative, indicating a strong electronic origin of nematicity linked to Fermi surface topology and quantum criticality.

ABSTRACT

We report on the synthesis and physical properties of FeSe$_{1-x}$Te$_x$ single crystals with a low Te content (x = 0.17, 0.21, 0.25), where the replacement of Se with Te partially suppresses superconductivity. Resistivity and Hall effect measurements indicate weak anomalies at elevated temperatures ascribed to nematic transitions. A quasi-classical analysis of transport data, including in a pulsed magnetic field of up to 25 T, confirms the inversion of majority carriers type from holes in FeSe to electrons in FeSe$_{1-x}$Te$_x$ at x $>$ 0.17. The temperature-dependent term in the elastoresistance of the studied compositions has a negative sign, which means that for substituted FeSe compositions, the elastoresistance is positive for hole-doped materials and negative for electron-doped materials just like in semiconductors such as silicon and germanium.

Motivation & Objective

  • To synthesize high-quality FeSe1-xTe x single crystals with low Te content (x < 0.3) to complete the nematic phase diagram of FeSe-based systems.
  • To investigate the emergence of nematic order and its interplay with electronic transport in FeSe1-xTe x under chemical pressure.
  • To determine the carrier type inversion and elastoresistivity behavior in FeSe1-xTe x as a function of Te doping.
  • To explore the connection between nematicity, Fermi surface topology, and quantum criticality in iron-based superconductors.

Proposed method

  • High-quality FeSe1-xTe x single crystals were synthesized using a flux method at temperatures slightly above the decomposition point of FeSe to enhance Te solubility and diffusion.
  • Resistivity and Hall effect measurements were performed in magnetic fields up to 25 T to analyze carrier type and transport anisotropy.
  • Elastoresistivity was measured to probe the electronic response to strain, with the coefficient C^EL extracted from temperature-dependent resistivity under uniaxial strain.
  • A three-band model was used to fit the Hall and longitudinal resistivity data in magnetic fields (up to 25 T), enabling extraction of carrier concentrations and mobilities.
  • Energy-dispersive spectroscopy (EDS) was used to determine the actual Te content (x_EDS) in the crystals, confirming the nominal doping level.
  • The structural transition temperature T_N was identified from the derivative dρ_xx/dT, and superconducting T_c was extracted from ρ_xx(T) curves.

Experimental results

Research questions

  • RQ1Does low Te doping (x < 0.3) induce a nematic transition in FeSe1-xTe x, and at what temperature does it occur?
  • RQ2Does the carrier type in FeSe1-xTe x invert from hole-like to electron-like with increasing Te content, and at what x does this occur?
  • RQ3How does the sign of the elastoresistivity coefficient C^EL evolve with Te doping, and what does it reveal about the electronic nature of nematicity?
  • RQ4Is there a correlation between the nematic transition temperature T_N and the total carrier concentration n_∑ in FeSe1-xTe x?
  • RQ5Can the observed transport anomalies be explained by a quantum critical point near x ≈ 0.15, where the Fermi level crosses the Van Hove singularity?

Key findings

  • The nematic transition temperature T_N decreases from ~85 K in pure FeSe to ~70 K at x = 0.17, ~60 K at x = 0.21, and ~60 K at x = 0.25, indicating suppression of nematic order with Te doping.
  • A clear inversion of the majority carrier type from holes in FeSe to electrons in FeSe1-xTe x occurs at x > 0.17, confirmed by Hall effect and magnetotransport analysis.
  • The elastoresistivity coefficient C^EL has a negative sign in FeSe1-xTe x (x = 0.17, 0.21, 0.25), indicating negative elastoresistance, which is characteristic of electron-doped systems like Ge and Si.
  • For x = 0.17, the three-band fit yields n_h = 11.5×10^19 cm⁻³ (μ_h = 303 cm²/Vs), n_e1 = 11.9×10^19 cm⁻³ (μ_e1 = 343 cm²/Vs), and n_e2 = 0.32×10^19 cm⁻³ (μ_e2 = 1830 cm²/Vs).
  • For x = 0.21, the fit gives n_h = 13.3×10^19 cm⁻³ (μ_h = 152 cm²/Vs), n_e1 = 14.7×10^19 cm⁻³ (μ_e1 = 163 cm²/Vs), and n_e2 = 0.11×10^19 cm⁻³ (μ_e2 = 890 cm²/Vs), confirming electron dominance.
  • The local minimum in total carrier concentration n_∑ coincides with the local maximum in T_N, supporting the electronic origin of the nematic transition.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.