[Paper Review] Stability of a high-finesse optical cavity at 493 nm in vacuum for cavity QED with Barium ions
The paper investigates vacuum- and laser-induced degradation of high-finesse oxide-coated mirrors at 493 nm, assessing viability for Ba+ cavity QED and identifying laser-induced deposition as a likely damage mechanism.
We explore the stability of a high-finesse optical cavity at 493 nm in vacuum for cavity QED with Barium ions. A high-finesse Fabry-Perot cavity is built using mirrors with high-reflectivity (HR) coatings that are implemented by stacking multiple thin films of low-loss dielectrics on substrates. Applications of such HR mirrors in the near ultraviolet (UV) range have been hampered by degradation of coatings in vacuum. Here, we explore the degradation of mirrors with HR coatings at 493 nm in vacuum. We study both vacuum-induced and laser-induced effects on oxide-coated cavity mirrors by probing changes in cavity loss using cavity lifetime measurements. We investigate the role of circulating power in the rate of increase in cavity loss and demonstrate methods of reversal of cavity degradation. While we observe no degradation without long exposure or with short exposures at lower circulating powers, we find evidence of degradation on long exposure to high circulating powers. We discuss potential causes and conclude that laser-induced deposition is the likely cause while ruling out thermally activated processes due to laser-induced heating.
Motivation & Objective
- Assess whether HR oxide-coated mirrors at 493 nm degrade in ultra-high vacuum over long durations.
- Determine whether vacuum-induced oxygen depletion or laser exposure drives degradation.
- Quantify cavity loss/finesse changes under varying circulating powers and exposure times.
- Investigate recovery mechanisms and potential mitigation for Ba+ cavity QED applications at 493 nm.
Proposed method
- Construct a 12.7 mm, 1,000 mm radius-of-curvature Fabry-Perot cavity with HR493 mirrors.
- Measure cavity lifetime and infer loss from ringdown transients (P_PD(t) ~ exp(-t/τ)).
- Operate at ~493.4 nm with a 493 nm laser and a stabilized 986 nm laser doubled to 493 nm to probe the cavity.
- Monitor cavity loss over months under vacuum (∼2×10^-8 mbar) with careful control of circulating power.
- Test two degradation scenarios: vacuum-induced (oxygen depletion) and laser-induced (hydrocarbon deposition).
- Analyze mode-dependence of degradation by comparing TEM00, TEM01, and TEM11 ringdowns to locate damage.
Experimental results
Research questions
- RQ1Does prolonged vacuum exposure cause oxide mirror degradation at 493 nm relevant to Ba+ cavity QED?
- RQ2Is laser-induced deposition the dominant mechanism for degradation at high circulating powers at 493 nm?
- RQ3How does circulating power affect the rate of cavity loss, and is there a power threshold for damage?
- RQ4Can degradation be reversed by oxygen exposure, and does 397 nm irradiation accelerate recovery?
Key findings
- Vacuum-induced degradation is negligible over months; loss rate is consistent with zero within measurement error (0.4±1.5)×10^-4 ppm/hour.
- Laser-induced degradation appears at high circulating powers and prolonged exposure, increasing cavity loss from ~30 ppm to >130 ppm over ~800 hours.
- Damage appears localized to the irradiated spot and shows lower loss for higher-order modes, indicating laser-induced surface damage rather than uniform diffusion.
- Recovery of finesse is accelerated by exposure to 397 nm light and oxygen exposure, with partial or complete restoration observed after air introduction.
- Thermally activated processes are unlikely to be the primary cause of degradation, given inconsistent power dependence and top-layer composition (silica on Ta2O5/SiO2).
- The results support feasibility of low-photon-number cavity QED with Ba+ at 493 nm, but highlight locking and damage concerns at high intra-cavity powers.
Read this paper
Open the full text in the Nubint reader and ask about any passage as you read.
Read this paper on NubintThis review was generated by AI from the original paper. Please check the paper before citing it.