[Paper Review] Superconductivity of FeSe$_{1-x}$Te$_{x}$ Thin Films Grown by Pulsed Laser Deposition
This study demonstrates the growth of FeSe$_{1-x}$Te$_{x}$ thin films via pulsed laser deposition on MgO(100) and LaSrAlO$_{4}$(001) substrates, achieving superconducting transitions at 6.7 K (onset) and 5.5 K (zero resistivity) on MgO, while films on LaSrAlO$_{4}$ show only a 2.6 K onset without zero resistivity, highlighting the critical role of epitaxial strain in tuning superconducting properties.
FeSe$_{1-x}$Te$_{x}$ thin films with PbO-type structure are successfully grown on MgO(100) and LaSrAlO$_{4}$(001) substrates from FeSe$_{1-x}$Te$_{x+d}$ polycrystalline targets by pulsed-laser deposition. The film deposited on the MgO substrate (film thickness $\sim$ 63 nm) shows superconductivity at 6.7 K (onset) and 5.5 K (zero resistivity). On the other hand, the film deposited on the LaSrAlO$_{4}$ substrate (film thickness $\sim$ 52 nm) exhibits only the onset of superconducting transition at 2.6 K, but does not show zero resistivity. This indicates the strong influence of epitaxial strain to superconducting properties of FeSe$_{1-x}$Te$_{x}$ thin films.
Motivation & Objective
- To grow high-quality FeSe$_{1-x}$Te$_{x}$ thin films with PbO-type structure using pulsed laser deposition.
- To investigate the influence of epitaxial strain from different substrates on superconducting properties.
- To determine the critical role of substrate lattice mismatch in modulating superconducting transition temperature and zero-resistivity behavior.
- To compare superconducting performance between films grown on MgO(100) and LaSrAlO$_{4}$(001) substrates.
Proposed method
- Pulsed laser deposition was used to grow FeSe$_{1-x}$Te$_{x}$ thin films from polycrystalline FeSe$_{1-x}$Te$_{x+d}$ targets.
- Epitaxial thin films were grown on MgO(100) and LaSrAlO$_{4}$(001) substrates to control lattice strain.
- Film thickness was measured at approximately 63 nm on MgO and 52 nm on LaSrAlO$_{4}$.
- Electrical resistivity measurements were performed to identify superconducting transitions and zero-resistivity onset.
- Structural quality was confirmed via X-ray diffraction and film orientation analysis.
Experimental results
Research questions
- RQ1How does epitaxial strain from different substrates affect the superconducting transition temperature in FeSe$_{1-x}$Te$_{x}$ thin films?
- RQ2What is the impact of substrate lattice mismatch on the emergence of zero resistivity in FeSe$_{1-x}$Te$_{x}$ thin films?
- RQ3Can pulsed laser deposition produce high-quality FeSe$_{1-x}$Te$_{x}$ thin films with PbO-type structure on various oxide substrates?
- RQ4Why does the film on LaSrAlO$_{4}$ show only a transition onset at 2.6 K without reaching zero resistivity?
Key findings
- The FeSe$_{1-x}$Te$_{x}$ film grown on MgO(100) exhibited a superconducting transition onset at 6.7 K and zero resistivity at 5.5 K.
- The film on LaSrAlO$_{4}$(001) showed a transition onset at 2.6 K but did not achieve zero resistivity, indicating suppressed superconductivity.
- The difference in superconducting behavior is attributed to the distinct epitaxial strain induced by the two substrates.
- The results demonstrate that epitaxial strain significantly modulates superconducting properties in FeSe$_{1-x}$Te$_{x}$ thin films.
- Pulsed laser deposition successfully produced phase-pure, epitaxial FeSe$_{1-x}$Te$_{x}$ thin films with PbO-type structure on both substrates.
Read this paper
Open the full text in the Nubint reader and ask about any passage as you read.
Read this paper on NubintThis review was generated by AI from the original paper. Please check the paper before citing it.