[Paper Review] A study on the mechanical property and corrosion sensitivity of an AA5086 friction stir welded joint
This study investigates the mechanical properties and corrosion sensitivity of friction stir-welded AA5086 joints, revealing that the thermo-mechanically affected zone (TMAZ)/heat-affected zone (HAZ) exhibits the lowest microhardness and is the primary failure site in tensile testing. Corrosion testing showed the HAZ had the lowest corrosion rate in 3.15 wt.% NaCl, with decreasing corrosion severity from 3.15% NaCl to ASTM seawater and then to 0.5 M Na2SO4, supported by SEM, XRD, and Raman analysis of corrosion products.
The mechanical property and corrosion sensitivity of a friction stir welded (FSW) AA5086 joint have been investigated. Vickers microhardness and tensile tests showed that the TMAZ/HAZ zone had the lowest microhardness value and the tensile specimen (transverse to the weld) failed in this region. Polarization experiments conducted using samples cut from each zone indicated that the HAZ had the lowest corrosion rate in 3.15 wt.% NaCl. SEM observation of the samples, Raman spectroscopic and XRD characterization of the corrosion products, and weight loss analysis after immersion tests all showed that the corrosion severity of AA5086 decreased from 3.15% NaCl to ASTM seawater and finally to 0.5 M Na2SO4. In addition, less corrosion products were observed from HAZ as compared to the other three regions, which was in agreement with the Raman and XRD analyses.
Motivation & Objective
- To evaluate the mechanical performance of friction stir-welded AA5086 joints, particularly focusing on microhardness and tensile strength distribution.
- To assess the corrosion sensitivity of different zones (TMAZ, HAZ, base metal, and weld nugget) in AA5086 after friction stir welding.
- To compare corrosion behavior across varying electrolytes: 3.15 wt.% NaCl, ASTM seawater, and 0.5 M Na2SO4.
- To correlate microstructural features with electrochemical and surface analysis results to understand corrosion mechanisms.
Proposed method
- Vickers microhardness testing was performed across distinct zones of the FSW joint to map hardness distribution.
- Tensile testing of transverse specimens was conducted to determine failure location and mechanical response.
- Electrochemical polarization tests were carried out on samples extracted from each zone to measure corrosion rates.
- Scanning electron microscopy (SEM) was used to examine surface morphology of corroded samples.
- X-ray diffraction (XRD) and Raman spectroscopy were applied to identify corrosion product phases.
- Weight loss measurements after immersion tests were used to quantify corrosion severity across different environments.
Experimental results
Research questions
- RQ1Which zone in the FSW AA5086 joint exhibits the lowest microhardness and is most prone to tensile failure?
- RQ2How does the corrosion rate vary across different zones of the FSW joint in 3.15 wt.% NaCl solution?
- RQ3What is the relative corrosion severity of the joint in 3.15% NaCl, ASTM seawater, and 0.5 M Na2SO4 electrolytes?
- RQ4How do the composition and morphology of corrosion products differ between zones and environments?
- RQ5What is the relationship between microstructural zones and corrosion product formation in FSW AA5086 joints?
Key findings
- The TMAZ/HAZ region exhibited the lowest microhardness value, and tensile specimens fractured at this location.
- The HAZ showed the lowest corrosion rate in 3.15 wt.% NaCl, indicating reduced susceptibility to corrosion compared to other zones.
- Corrosion severity decreased in the order: 3.15% NaCl > ASTM seawater > 0.5 M Na2SO4, as confirmed by weight loss and surface analysis.
- Less corrosion product formation was observed in the HAZ compared to other zones, consistent with electrochemical and spectroscopic data.
- Raman and XRD analyses confirmed the presence of specific corrosion products, with variations in phase composition across zones and environments.
- The combined use of SEM, XRD, and Raman spectroscopy provided clear evidence of reduced corrosion in the HAZ and varying corrosion product characteristics across electrolytes.