Skip to main content
QUICK REVIEW

[Paper Review] Coking-Resistant Sub-Nano Dehydrogenation Catalysts: Pt$_n$Sn$_x$/SiO$_2$ (n = 4, 7)

Timothy J. Gorey, Borna Zandkarimi|arXiv (Cornell University)|Mar 10, 2020
Catalysis and Oxidation ReactionsChemical Engineering4 citations
TL;DR

This study presents PtₙSnₓ/SiO₂ (n = 4, 7) sub-nano cluster catalysts engineered to resist coking and sintering during hydrocarbon dehydrogenation. By alloying Pt clusters with Sn via selective H₂/SnCl₄ deposition, the catalysts suppress di-σ ethylene binding and dehydrogenation pathways, lowering the barrier for ethane-to-ethylene conversion while eliminating carbon deposition and cluster aggregation.

ABSTRACT

We present a combined experimental/theoretical study of Pt<sub><i>n</i></sub>/SiO<sub>2</sub> and Pt<sub><i>n</i></sub>Sn<sub><i>x</i></sub>/SiO<sub>2</sub> (<i>n</i> = 4, 7) model catalysts for the endothermic dehydrogenation of hydrocarbons, using the ethylene intermediate as a model reactant. Mass-selected Pt<sub><i>n</i></sub> clusters were deposited onto amorphous SiO<sub>2</sub>/Si­(100) to make the Pt<sub><i>n</i></sub>SiO<sub>2</sub> model catalysts. To produce Pt<sub><i>n</i></sub>Sn<sub><i>x</i></sub> clusters, size-selected Pt<sub><i>n</i></sub> was used to seed selective deposition of Sn on Pt via a self-limiting H<sub>2</sub>/SnCl<sub>4</sub>/H<sub>2</sub> reaction sequence. Model catalysts were analyzed using C<sub>2</sub>D<sub>4</sub> and CO temperature-programmed desorption (TPD), low-energy ion scattering (ISS), X-ray photoelectron spectroscopy (XPS), plane wave density functional theory (DFT) global optimization combined with a statistical mechanical description of the catalytic interface, and a DFT mechanistic study. Supported pure Pt<sub><i>n</i></sub> clusters are found to be highly active toward dehydrogenation of C<sub>2</sub>D<sub>4</sub>, quickly deactivating due to a combination of carbon deposition and sintering, resulting in loss of accessible Pt sites. Addition of Sn to Pt<sub><i>n</i></sub> clusters results in the complete suppression of C<sub>2</sub>D<sub>4</sub> dehydrogenation and carbon deposition and also stabilizes the clusters against thermal sintering. Theory shows that both systems have thermal access to a multitude of cluster structures and adsorbate configurations that form a statistical ensemble. While Pt<sub>4</sub>/SiO<sub>2</sub> clusters bind ethylene in both di-σ- and π-bonded configurations, Pt<sub>4</sub>Sn<sub>3</sub>/SiO<sub>2</sub> binds C<sub>2</sub>H<sub>4</sub> only in the π mode, with di-σ bonding suppressed by a combination of electronic and geometric features of the PtSn clusters. Dehydrogenation reaction profiles on the accessible cluster isomers were calculated using the climbing image nudged elastic band (CI-NEB) method. Dehydrogenation of di-σ-bound ethylene is computed to dominate and is suppressed by Sn addition, in agreement with the experiments. DFT indicates that, after Sn alloying, the barrier for ethane-to-ethylene conversion is lower than that for unwanted ethylene dehydrogenation.

Motivation & Objective

  • To develop coking-resistant sub-nano Pt-based catalysts for endothermic hydrocarbon dehydrogenation.
  • To understand how Sn alloying modifies the adsorption geometry and reactivity of ethylene on Pt clusters.
  • To stabilize Pt clusters against thermal sintering and carbon deposition under reaction conditions.
  • To elucidate the electronic and geometric origins of enhanced catalytic selectivity and stability in Pt-Sn clusters.
  • To bridge experimental observations with DFT modeling of cluster fluxionality and reaction pathways.

Proposed method

  • Mass-selected Pt₄ and Pt₇ clusters were deposited onto amorphous SiO₂/Si(100) substrates to form model catalysts.
  • Sn was selectively deposited onto pre-formed Pt clusters using a self-limiting H₂/SnCl₄ reaction sequence to form PtₙSnₓ clusters.
  • Temperature-programmed desorption (TPD) with C₂D₄ and CO probed surface reactivity and adsorption states.
  • Low-energy ion scattering (ISS) and X-ray photoelectron spectroscopy (XPS) characterized surface composition and oxidation states.
  • Plane-wave DFT global optimization identified stable cluster isomers and adsorbate configurations.
  • Climbing image nudged elastic band (CI-NEB) methods computed reaction barriers for ethylene dehydrogenation pathways.

Experimental results

Research questions

  • RQ1How does Sn alloying alter the adsorption geometry of ethylene on sub-nano Pt clusters?
  • RQ2What is the role of Sn in suppressing carbon deposition and cluster sintering during dehydrogenation?
  • RQ3How do electronic and geometric effects in PtₙSnₓ clusters influence the relative barriers for ethane-to-ethylene conversion versus ethylene dehydrogenation?
  • RQ4To what extent do cluster fluxionality and multiple isomeric structures contribute to catalytic behavior?
  • RQ5Can DFT modeling accurately predict the suppression of di-σ bonding and coking pathways in Pt-Sn systems?

Key findings

  • Pure Pt₄/SiO₂ and Pt₇/SiO₂ clusters rapidly deactivate due to carbon deposition and sintering during C₂D₄ dehydrogenation.
  • Pt₄Sn₃/SiO₂ clusters show complete suppression of ethylene dehydrogenation and carbon deposition, with no detectable coking.
  • Sn alloying stabilizes clusters against thermal sintering, preserving active site dispersion.
  • DFT calculations show that Pt₄Sn₃/SiO₂ binds ethylene exclusively in π-mode, with di-σ bonding suppressed by electronic and geometric effects.
  • The reaction barrier for ethane-to-ethylene conversion is lower than that for ethylene dehydrogenation on Pt₄Sn₃/SiO₂, favoring desired product formation.
  • Thermal access to multiple cluster isomers and adsorbate configurations creates a statistical ensemble, with Sn shifting the dominant pathway away from coking.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.