Skip to main content
QUICK REVIEW

[Paper Review] Combining laser ablation and Sol-Gel techniques for the synthesis of nanostructured organic-inorganic matrices

E. Haro-Poniatowski, C. A. Guarín|arXiv (Cornell University)|Jan 15, 2026
Laser-Ablation Synthesis of NanoparticlesEngineering0 citations
TL;DR

The paper reports a combined PLAL and Sol-Gel method to embed Au nanoparticles in glass and gelatin matrices, yielding transparent glasses and flexible gelatin films with distinct optical properties.

ABSTRACT

In this work we report a new and simple method that combines the pulsed laser ablation in liquids (PLAL) and the Sol-Gel techniques to obtain nanocomposite glasses and gelatins. Gold nanoparticles (Au-NPs) are generated by PLAL using the corresponding target. The target is submerged in a transparent liquid solution made previously with tetraetylorthosilicate (TEOS) adding diluted hydrochloric acid as catalyzer. In the case of gelatins commercial gelatin and tap water are used. The laser source is a Nd:YAG laser emitting at 1064 nm, with an energy of 100 mJ and 8 ns pulse duration at 10 Hz repetition rate focused on the target in a 2 mm diameter laser spot. The ablation time is 10 min for the glasses and gelatins. The Au-NPs are uniformly dispersed in the solution. After the ablation process the gels are sealed and stored at room temperature for several days. The samples are characterized by UV-Vis spectroscopy, HRTEM, ellipsometry and AFM microscopy, these measurements reveal optical transparency and a refractive index near 1.45 for the pure glass, whereas a colorful aspect, a refractive index of 1.42, and a small surface roughness of 1.92 nm for the glass containing Au-NPs. In the case of gelatins self-sustained flexible films are obtained.

Motivation & Objective

  • Develop a simple combined PLAL-Sol-Gel synthesis route for nanocomposite glasses and gelatins.
  • Generate gold nanoparticles via PLAL and disperse them uniformly in TEOS-based solutions.
  • Produce transparent glass matrices and self-sustained gelatin films with embedded Au-NPs.

Proposed method

  • Use a Nd:YAG laser at 1064 nm with 100 mJ energy, 8 ns pulse duration, 10 Hz repetition rate, focused to a 2 mm spot on the target.
  • Submerge the target in TEOS solution with diluted HCl as a catalyst to form the gel/sol matrix.
  • Perform ablation for 10 minutes to generate Au-NPs and distribute them in the solution or gel.
  • Characterize samples with UV-Vis spectroscopy, HRTEM, ellipsometry, and AFM to assess optical and surface properties.
  • Store the resulting gels at room temperature for several days to mature the matrices.

Experimental results

Research questions

  • RQ1Can PLAL-generated Au-NPs be uniformly dispersed in TEOS-based gels and glasses using a Sol-Gel process?
  • RQ2What are the optical and surface-property changes induced by embedding Au-NPs in the Sol-Gel matrices?
  • RQ3Do the resulting materials form transparent glasses and self-supported gelatin films with desirable nanostructure?
  • RQ4How do synthesis parameters (laser energy, ablation time, catalyst concentration) affect NP dispersion and matrix properties?

Key findings

  • Glass matrices show optical transparency with a refractive index near 1.45 for the pure glass.
  • Glass matrices with Au-NPs exhibit a refractive index of 1.42 and a small surface roughness of 1.92 nm.
  • Gelatin-based samples form self-sustained flexible films.
  • Au-NPs are uniformly dispersed in the solution after ablation.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.