Skip to main content
QUICK REVIEW

[Paper Review] Enhancing surface production of negative ions using nitrogen doped diamond in a deuterium plasma

Gregory J Smith, James Ellis|arXiv (Cornell University)|Jul 1, 2020
Diamond and Carbon-based Materials ResearchMaterials Science73 references11 citations
TL;DR

This study demonstrates that nitrogen-doped microcrystalline diamond (MCNDD) enhances surface production of negative ions in a deuterium plasma, particularly under low-energy ion bombardment. At 550 °C and -20 V bias, MCNDD increases negative ion yield by a factor of 2 over undoped diamond and 1.5 over boron-doped diamond, offering a promising alternative to caesium-coated surfaces in fusion applications.

ABSTRACT

The production of negative ions is of significant interest for applications including mass spectrometry, particle acceleration, material surface processing, and neutral beam injection for magnetic confinement fusion. Methods to improve the efficiency of the surface production of negative ions, without the use of low work function metals, are of interest for mitigating the complex engineering challenges these materials introduce. In this study we investigate the production of negative ions by doping diamond with nitrogen. Negatively biased ($-20$ V or $-130$ V), nitrogen doped micro-crystalline diamond films are introduced to a low pressure deuterium plasma (helicon source operated in capacitive mode, 2 Pa, 26 W) and negative ion energy distribution functions (NIEDFs) are measured via mass spectrometry with respect to the surface temperature (30$^{\\circ}$C to 750$^{\\circ}$C) and dopant concentration. The results suggest that nitrogen doping has little influence on the yield when the sample is biased at $-130$ V, but when a relatively small bias voltage of $-20$ V is applied the yield is increased by a factor of 2 above that of un-doped diamond when its temperature reaches 550$^{\\circ}$C. The doping of diamond with nitrogen is a new method for controlling the surface production of negative ions, which continues to be of significant interest for a wide variety of practical applications.

Motivation & Objective

  • To investigate nitrogen doping of microcrystalline diamond as a method to enhance surface production of negative ions in low-pressure deuterium plasma.
  • To evaluate the impact of nitrogen doping on negative ion yield under varying surface temperatures and applied bias voltages.
  • To compare the performance of nitrogen-doped diamond (MCNDD) with undoped (MCD) and boron-doped diamond (MCBDD) under identical plasma conditions.
  • To determine whether nitrogen doping can improve negative ion yield without relying on low work function metals like caesium.
  • To identify optimal temperature and bias conditions for maximizing negative ion production using doped diamond films.

Proposed method

  • Synthesis of microcrystalline diamond films (MCD) with nitrogen doping at 50 ppm via plasma-enhanced chemical vapor deposition (PECVD).
  • Exposure of doped and undoped diamond films to a low-pressure deuterium plasma (2 Pa, 26 W) generated by a helicon source in capacitive mode.
  • Application of variable negative DC bias (-20 V or -130 V) to the diamond samples to control ion energy and surface potential.
  • Measurement of negative ion energy distribution functions (NIEDFs) using mass spectrometry across a temperature range from 30 °C to 750 °C.
  • Systematic variation of film surface temperature to assess thermal activation effects on negative ion yield.
  • Comparison of negative ion yields across MCD, MCBDD, and MCNDD samples under identical plasma and bias conditions.

Experimental results

Research questions

  • RQ1Does nitrogen doping of microcrystalline diamond enhance negative ion yield in a deuterium plasma compared to undoped or boron-doped diamond?
  • RQ2How does the applied bias voltage (-20 V vs. -130 V) influence the effectiveness of nitrogen doping in boosting negative ion production?
  • RQ3At what temperature does nitrogen-doped diamond exhibit peak negative ion yield, and how does this compare to undoped and boron-doped diamond?
  • RQ4What is the role of surface temperature in modulating the resonant charge transfer process in doped diamond films?
  • RQ5Can nitrogen-doped diamond serve as a viable, caesium-free alternative for negative ion sources in magnetic confinement fusion applications?

Key findings

  • At -20 V bias and 550 °C, nitrogen-doped microcrystalline diamond (MCNDD) produces a negative ion yield 2× higher than undoped diamond (MCD).
  • At the same conditions, MCNDD yields 1.5× more negative ions than boron-doped microcrystalline diamond (MCBDD), the previously best-performing material.
  • Under high-energy ion bombardment (-130 V), nitrogen doping shows no significant yield enhancement over undoped diamond, indicating bias-dependent effectiveness.
  • The negative ion yield for MCNDD increases by several orders of magnitude between 400 °C and 550 °C, peaking at 550 °C before declining.
  • Below 400 °C, MCNDD shows negligible negative ion yield, suggesting a thermal activation threshold for the doping effect.
  • The yield trends for MCD and MCBDD are consistent with prior studies, validating the experimental setup and baseline performance.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.