Skip to main content
QUICK REVIEW

[Paper Review] Facilitating electrical and laser-induced skyrmion nucleation with a dipolar-field enhanced effective DMI

Mark C. H. de Jong, D. I. Khusyainov|arXiv (Cornell University)|Feb 2, 2026
Magnetic properties of thin filmsPhysics and Astronomy0 citations
TL;DR

The paper demonstrates that engineering layer-dependent DMI signs in Ir/Co/Pt multilayers to align dipolar and DMI fields enhances the effective DMI, markedly increasing skyrmion nucleation density for both current-driven and laser-induced methods while leaving thresholds largely unchanged.

ABSTRACT

We demonstrate experimentally how the nucleation of skyrmions in an Ir, Co, and Pt based magnetic multilayer is affected by introducing a layer dependent sign for the Dzyaloshinskii-Moriya interaction (DMI). In one stack, the bottom half of the stack is given a positive DMI and the top half a negative DMI, and as a result, the in-plane component of the dipolar field is aligned parallel to the effective field of the DMI in every layer, enhancing the effective DMI. We show that this enhanced DMI facilitates the nucleation and stability of skyrmions using both current-driven and laser-induced skyrmion nucleation. In the devices with an enhanced effective DMI, the density of nucleated skyrmions is greater by up to a factor 20 and skyrmions can be observed in stronger magnetic fields - suggesting that their stability is also improved. These results show that skyrmion nucleation depends strongly on the magnitude of the effective DMI in a magnetic multilayer and that the dipolar field within such a multilayer presents an effective route towards controlling the effective DMI, and thereby, the nucleation of chiral magnetic textures.

Motivation & Objective

  • Motivate control of skyrmion chirality and stability via the DMI in magnetic multilayers.
  • Investigate how dipolar fields modify the effective DMI in multilayers with layer-dependent DMI signs.
  • Compare current-driven and laser-induced skyrmion nucleation under enhanced vs reduced effective DMI.
  • Quantify changes in skyrmion density and stability due to dipolar-field engineering while keeping other parameters constant.

Proposed method

  • Fabricate four multilayer stacks with distinct DMI configurations: Uniform+ and Uniform−, Enhanced, and Reduced.
  • Measure saturation magnetization and uniaxial anisotropy to ensure comparable M_s and K_u across stacks.
  • Determine effective DMI by analyzing equilibrium domain widths using Lemesh et al.'s model.
  • Perform current-driven skyrmion nucleation using nanosecond pulses and map density via MFM.
  • Perform laser-induced skyrmion nucleation with 70 fs pulses and map density via MFM.
  • Simulate dipolar-DMI interplay with MuMax3 and compare to analytical models.
Figure 1: Sketches of the different multilayer structures. (a) Uniform $+$ stack. All the layers in this stack have a positive DMI sign. (b) Uniform $-$ stack. Same as (a), but with the opposite DMI sign. (c) Enhanced stack. Here the magnetic layers in the top half of the stack have a negative DMI a
Figure 1: Sketches of the different multilayer structures. (a) Uniform $+$ stack. All the layers in this stack have a positive DMI sign. (b) Uniform $-$ stack. Same as (a), but with the opposite DMI sign. (c) Enhanced stack. Here the magnetic layers in the top half of the stack have a negative DMI a

Experimental results

Research questions

  • RQ1How does aligning dipolar fields with the DMI effective field across layers modify the overall effective DMI in a multilayer?
  • RQ2Does an enhanced effective DMI enable higher skyrmion nucleation densities for both current-driven and laser-induced excitation without significantly altering nucleation thresholds?
  • RQ3How do the enhanced and reduced stacks compare in skyrmion stability and density under varying bias fields and excitation fluences?

Key findings

  • The enhanced stack exhibits an effective DMI about 2.5 times larger than the reduced stack, with similar M_s and K_u across stacks.
  • Skyrmion density after current-driven nucleation is ~20 times higher in the enhanced stack than in the reduced stack (10.6(1) vs 0.52(1) per μm^2).
  • The nucleation threshold current densities are similar between enhanced and reduced stacks (approximately 7.09(1)×10^11 A/m^2 vs 6.90(2)×10^11 A/m^2).
  • Laser-induced nucleation shows higher skyrmion densities in the enhanced stack across fluences, with a higher saturation density and a fourfold increase in saturation density relative to the reduced stack.
  • Threshold fluences for laser nucleation are Fc = 9.0(2) and 10.7(2) mJ/cm^2 for enhanced and reduced stacks, respectively.
  • Measured ΔDMI between enhanced and reduced stacks ≈ 0.6 mJ/m^2 (enhanced) and 0.47(6) mJ/m^2 (measured difference), consistent with dipolar-origin predictions.
Figure 3: Effect of the enhanced and reduced effective DMI on the current- and laser-induced nucleation of skyrmions. In (a) - (l) we show MFM scans of the magnetization in the devices fabricated from the enhanced and reduced multilayer stack after applying a single nucleation pulse. (a) - (c): Enha
Figure 3: Effect of the enhanced and reduced effective DMI on the current- and laser-induced nucleation of skyrmions. In (a) - (l) we show MFM scans of the magnetization in the devices fabricated from the enhanced and reduced multilayer stack after applying a single nucleation pulse. (a) - (c): Enha

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.