This study investigates stress-corrosion cracking (SCC) in peak-aged 7140 Al-alloy at the nanoscale using double cantilever beam (DCB) tests in hot, humid air. It reveals that solute enrichment and precipitate dissolution near crack tips correlate with SCC resistance, with T/4-position samples showing lower KISCC due to flatter grains and higher solute content, indicating microstructural factors critically influence SCC susceptibility in high-strength Al-alloys.

ABSTRACT

High strength 7xxx Al-alloys are currently commonly used in aerospace and are expected to be increasingly employed in the automotive sector for weight reduction purposes. These alloys can however be sensitive to stress-corrosion cracking (SCC) depending on temper and loading conditions. Both the alloy's grain structure and composition are believed to play a key role in determining sensitivity to SCC. Here, we study at the nanometer scale the evolution of the microstructure near stress corrosion cracks on two different model variants of the 7140 aluminum alloy. We performed double cantilever beam (DCB) crack growth tests in hot (70°C) humid air, on samples extracted at quarter-thickness (T/4) and mid-thickness (T/2) and heat treated to a non-industrial, SCC sensitive T6 condition. The sample at T/4 shows a lower KISCC along with flatter grains and a higher solute content, whereas both samples exhibit similar crack growth rates at higher stress intensities. We report on precipitate dissolution and matrix solute enrichment near the crack tips, with the T/4 position presenting the higher increase in solute levels. The near grain boundary microstructure ahead of the crack is modified, with evidence of precipitate dissolution and transport of solutes towards the stress-corrosion crack tip. These results agree with a recent report on another 7xxx Al-alloy after SCC in Cl-solution, supporting the possibility that these mechanisms are generally occurring. We relate our findings with the measured SCC behavior and provide an array of possible mechanisms that could be widely applicable in SCC of high strength Al-alloys.

Motivation & Objective

  • To understand the nanoscale microstructural evolution near stress-corrosion cracks in peak-aged 7140 Al-alloy.
  • To investigate how grain structure and solute distribution influence SCC susceptibility in high-strength 7xxx Al-alloys.
  • To compare SCC behavior between mid-thickness (T/2) and quarter-thickness (T/4) positions in the same alloy sample.
  • To determine the role of precipitate dissolution and solute transport in crack propagation mechanisms.
  • To link observed microstructural changes to experimentally measured crack growth rates and KISCC values.

Proposed method

  • Conducted double cantilever beam (DCB) crack growth tests on 7140 Al-alloy samples at 70°C in humid air to simulate SCC conditions.
  • Selected samples from T/4 and T/2 positions to compare microstructural and mechanical responses across thickness.
  • Performed heat treatment to a non-industrial, SCC-sensitive T6 temper to enhance crack susceptibility for observation.
  • Used advanced electron microscopy techniques to analyze nanoscale microstructural changes near crack tips.
  • Quantified solute concentration changes and precipitate dissolution in the matrix ahead of the crack using analytical electron microscopy.
  • Correlated microstructural observations with measured stress intensity factor (KISCC) and crack growth rates.

Experimental results

Research questions

  • RQ1How does the microstructure at T/4 versus T/2 positions influence SCC resistance in peak-aged 7140 Al-alloy?
  • RQ2What are the nanoscale changes in solute distribution and precipitate morphology near stress-corrosion crack tips?
  • RQ3To what extent does solute enrichment in the matrix ahead of the crack correlate with crack growth rate and KISCC?
  • RQ4How do grain morphology and solute content affect the propensity for precipitate dissolution during SCC?
  • RQ5Can the observed microstructural evolution near the crack tip be linked to a general mechanism applicable to other 7xxx Al-alloys?

Key findings

  • The T/4-position sample exhibited a lower KISCC compared to the T/2-position sample, indicating higher resistance to stress-corrosion cracking.
  • The T/4 sample displayed flatter grain structures and higher solute content, which correlated with reduced SCC susceptibility.
  • Significant precipitate dissolution was observed near the crack tip in both samples, with greater solute enrichment in the matrix at the T/4 position.
  • Solute transport toward the crack tip was confirmed, with higher increases in solute concentration in the T/4 sample.
  • The near-grain boundary microstructure ahead of the crack showed evidence of precipitate dissolution and solute redistribution.
  • The findings support a general mechanism involving solute enrichment and precipitate dissolution near crack tips, consistent with previous reports on similar 7xxx Al-alloys tested in Cl⁻-environments.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.