This study establishes a comprehensive growth diagram for InAlN alloys grown by plasma-assisted molecular beam epitaxy (PA-MBE), revealing how indium incorporation and surface morphology depend on growth temperature and indium flux. By quantifying InN decomposition via Arrhenius behavior (Ea = 2.0 eV) and In desorption, the authors define four distinct growth regimes—N-rich, In-droplets, intermediate In-rich, and negligible In incorporation—enabling precise control over alloy composition and surface quality.
Indium incorporation and surface morphology of InAlN layers grown on (0001)GaN by plasma-assisted molecular beam epitaxy were investigated as a function of the impinging In flux and the substrate temperature in the 450-610$^{\circ}$C range. In incorporation was found to decrease with substrate temperature due to thermal decomposition of the growing layer, while for a given temperature it increased with the impinging In flux until stoichiometry was reached at the growth front. The InN losses during growth followed an Arrhenius behaviour characterized by an activation energy of 2.0 eV. A growth diagram highly instrumental to identify optimum growth conditions was established.
Motivation & Objective
- To understand the dependence of In incorporation and surface morphology in InAlN layers on growth temperature and indinging In flux.
- To identify the dominant mechanisms limiting In incorporation, particularly thermal decomposition of InN and In desorption.
- To develop a practical growth diagram that guides optimal growth conditions for high-quality InAlN alloys.
- To enable precise control over InN mole fraction and surface morphology in InAlN epilayers for optoelectronic and electronic device applications.
Proposed method
- Measured In incorporation via high-resolution X-ray diffraction (HR-XRD) to determine actual InN mole fraction [InN]*.
- Used beam equivalent pressure (BEP) calibration with cross-sectional SEM to quantify metal and nitrogen fluxes in atoms/cm²·s.
- Constructed an Arrhenius plot of InN loss rates to extract activation energy (Ea = 2.0 eV) for thermal decomposition.
- Modeled InN loss using the equation Φlosses_InN = C·[InN]*·exp(-Ea/kBT), where C = 1.27×10²⁷ s⁻¹·cm².
- Defined growth regimes using two solid lines: one for stoichiometric conditions (ΦIn = ΦN - ΦAl + Φlosses_InN), and one for In desorption onset (ΦIn = ΦN - ΦAl + Φlosses_InN - Φdes_In).
- Characterized surface morphology via SEM and atomic force microscopy (AFM), identifying step-flow growth and smooth surfaces under specific conditions.
Experimental results
Research questions
- RQ1How does growth temperature affect indium incorporation in InAlN layers grown by PA-MBE?
- RQ2What is the role of InN thermal decomposition in limiting In incorporation, and what is its activation energy?
- RQ3How does the impinging In flux influence the achievable InN mole fraction and surface morphology?
- RQ4What growth regimes—defined by temperature and flux—yield smooth, high-quality InAlN surfaces with minimal defects?
- RQ5Can a predictive growth diagram be constructed to guide optimal growth conditions for InAlN alloys?
Key findings
- Indium incorporation in InAlN decreases with increasing growth temperature due to thermal decomposition of InN, with [InN]* dropping from 0.33 at 450 °C to 0.02 at 607 °C.
- The activation energy for InN decomposition was determined to be 2.0 eV, consistent with the In-N bond energy (1.93 eV) and prior measurements on InN.
- An Arrhenius behavior for InN loss rates was confirmed, with a pre-exponential factor of 1.27×10²⁷ s⁻¹·cm².
- Four distinct growth regimes were identified: N-rich, In-droplets, intermediate In-rich, and negligible In incorporation, with the intermediate In-rich regime yielding the smoothest surfaces (RMS < 0.8 nm).
- Smooth surfaces with atomic steps and spiral hillocks were observed in the intermediate In-rich regime, indicating dislocation-pinned step-flow growth similar to GaN under Ga-rich conditions.
- Surprisingly, N-rich growth also produced smooth surfaces (RMS < 0.8 nm), contrary to typical roughness under N-rich conditions in III-N semiconductors.