Skip to main content
QUICK REVIEW

[Paper Review] Case study of an exploratory high voltage NASICON-based Na$_4$NiCr(PO$_4$)$_3$ cathode material for sodium-ion batteries

Madhav Sharma, Pooja Sindhu|arXiv (Cornell University)|Jan 11, 2026
Advancements in Battery MaterialsEngineering0 citations
TL;DR

The paper analyzes Na4NiCr(PO4)3 (NNCP) within a NASICON framework as a high-voltage SIB cathode, revealing good Na+ diffusion pathways but irreversible electrochemical behavior due to poor electronic conductivity.

ABSTRACT

We examine a new NASICON-type Na$_4$NiCr(PO$_4$)$_3$ material designed for high-voltage and multi-electron reactions for the sodium-ion batteries (SIBs). The Rietveld refinement of the X-ray diffraction pattern, using the R$\bar{3}$c space group, confirmed the stabilization of the rhombohedral NASICON framework. Furthermore, the Raman and Fourier transform infrared spectroscopy are employed to probe the structure and chemical bonding. The core-level photoemission analysis reveals the Cr$^{3+}$ and mixed Ni$^{2+}$/Ni$^{3+}$ oxidation states in the sample. Moreover, the bond valence energy landscape (BVEL) analysis, based on the refined structure, revealed a three-dimensional network of well-connected sodium sites with a migration energy barrier of 0.468 eV. The material delivered a good charge capacity at around 4.5 V, but showed no sodium-ion intercalation during discharge, resulting in negligible discharge capacity. The post-mortem analysis confirmed that the crystal structure remained intact. The calculated energy barrier values indicated a reversal in sodium site stability after cycling, though the barriers can still permit feasible ion migration. This suggests that ion transport alone cannot explain the lack of reversibility, which likely arises from intrinsically poor electronic conductivity. These findings highlight key challenges in achieving stable, reversible capacity in this system and underscore the need for doping, structural modification, and electrolyte optimization to realize its full potential as a high-voltage SIB cathode.

Motivation & Objective

  • Motivate high-voltage cathodes for sodium-ion batteries using NASICON polyanionic frameworks.
  • Characterize structure and electronic states of NNCP to understand redox activity.
  • Assess Na+ diffusion pathways and migration barriers in NNCP.
  • Evaluate electrochemical reversibility and factors limiting capacity.
  • Propose routes (doping, coating, electrolyte) to improve performance.

Proposed method

  • Synthesize NNCP samples (air, Ar, with carbon coating) via sol-gel and calcination steps.
  • Perform Rietveld refinement of XRD data to confirm rhombohedral NASICON structure (R-3c).
  • Use Raman and FTIR to probe phosphate framework bonding.
  • Apply XPS to determine Cr and Ni oxidation states and their fractions.
  • Compute bond valence energy landscape (BVEL) from refined structure to map Na+ migration pathways and barriers.
  • Conduct electrochemical tests including EIS, CV, and galvanostatic charge-discharge on half-cells.
Figure 1: Rietveld-refined XRD patterns of (a) NNCP-Air, (b) NNCP-Ar, and (c) NNCP-Air/AB samples, and (d) crystal structure of NNCP-Air showing calculated iso-surfaces (in grey colour) for 3D Na + migration channels.
Figure 1: Rietveld-refined XRD patterns of (a) NNCP-Air, (b) NNCP-Ar, and (c) NNCP-Air/AB samples, and (d) crystal structure of NNCP-Air showing calculated iso-surfaces (in grey colour) for 3D Na + migration channels.

Experimental results

Research questions

  • RQ1What is the crystal structure and phase stability of NNCP in NASICON form?
  • RQ2What are the oxidation states and redox couples active at high voltage in NNCP?
  • RQ3Are Na+ diffusion pathways sufficiently connected and what are the migration barriers?
  • RQ4Is there reversible Na+ intercalation during cycling, and what limits reversibility?
  • RQ5Can strategies like carbon coating or synthesis atmosphere improve electronic conductivity and reversibility?

Key findings

  • NNCP-Air shows rhombohedral NASICON structure with lattice parameters a = b = 8.8165 Å, c = 21.2658 Å (space group R-3c).
  • BVEL analysis reveals a 3D interconnected Na+ diffusion network with a migration barrier of 0.468 eV.
  • Core-level XPS indicates Cr3+ and mixed Ni2+/Ni3+; oxygen vacancies balance Ni3+ for charge neutrality.
  • CV and GCD show high-voltage activity around 4.5 V (Cr3+/Cr4+), but no reversible Na+ intercalation; discharge capacity ~2–3 mAh/g.
  • DC polarization indicates extremely low electronic conductivity (6.57×10^-9 S/cm), contributing to irreversibility.
  • Post-cycling XRD shows preserved crystal structure with modest changes in Na-O and Ni/Cr–O bonds; energy landscape shifts after cycling (Na1/Na2 site stability changes).
  • Carbon coating (NNCP-Air/AB) lowers interfacial resistances but does not recover discharge reversibility; upper voltage limits did not restore reversibility.
Figure 2: (a) The Raman, (b) FTIR spectra, (c1) the FE-SEM image, (c2-c6) the EDS elemental mappings, and (d) the DC polarization curve at a voltage of 1 V of the NNCP-Air sample.
Figure 2: (a) The Raman, (b) FTIR spectra, (c1) the FE-SEM image, (c2-c6) the EDS elemental mappings, and (d) the DC polarization curve at a voltage of 1 V of the NNCP-Air sample.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.