TL;DR

The study shows Mn incorporation in GaN by plasma-assisted MBE is highest under N-rich conditions and lowest under Ga-rich conditions, with no-flux (Mn δ-doping) intermediate; Mn sticking coefficients relative to N-rich are 0.31 (no-flux) and 0.01 (Ga-rich).

ABSTRACT

This brief report examines the influence of Ga/N flux conditions on Mn incorporation in GaN. Mn-doped GaN layers were grown at 680$^{\circ}$C by molecular beam epitaxy on a Ga-polar GaN(0001) template substrate under Ga-rich, N-rich, and no-flux conditions (i.e., Mn $δ$ doping). Mn incorporation was highest under N-rich condition, lowest under Ga-rich condition, and intermediate in the absence of Ga and N fluxes. For the growth conditions examined in this study, the corresponding Mn sticking coefficients, relative to that of the N-rich condition, were determined to be 0.31 for no-flux growth and 0.01 for the Ga-rich growth.

Motivation & Objective

  • Examine how Ga/N flux conditions influence Mn incorporation in GaN grown by plasma-assisted MBE.
  • Quantify Mn incorporation levels under Ga-rich, N-rich, and no-flux (Mn δ-doping) growth.
  • Determine the relative Mn sticking coefficients under these flux regimes.
  • Understand the role of surface kinetics and cation-site competition in Mn incorporation.

Proposed method

  • Grow GaN:Mn/GaN multilayers on Ga-polar GaN(0001) templates at 680 °C under Ga-rich, N-rich, and no-flux conditions.
  • Maintain Mn beam flux constant while switching Ga and N fluxes to establish different growth regimes.
  • Use SIMS to profile Mn, O, C, H, and Si concentrations and estimate Mn areal densities.
  • Compute Mn incorporation fluxes from Mn shutter timings and SIMS profiles to derive relative sticking coefficients.
  • Compare Mn densities across regions to infer the dependence on Ga/N flux conditions.
Figure 1: (a) Schematic layer structure of GaN:Mn/GaN multilayers grown on a GaN template at 680 ∘ C by MBE. The double and single asterisks indicate growth interruptions of 12 min. and 6 min., respectively. (i)–(v) RHEED patterns taken along the $<$ 11 $\bar{2}$ 0 $>$ azimuth at various stages of t
Figure 1: (a) Schematic layer structure of GaN:Mn/GaN multilayers grown on a GaN template at 680 ∘ C by MBE. The double and single asterisks indicate growth interruptions of 12 min. and 6 min., respectively. (i)–(v) RHEED patterns taken along the $<$ 11 $\bar{2}$ 0 $>$ azimuth at various stages of t

Experimental results

Research questions

  • RQ1How does the Ga/N flux ratio during growth affect Mn incorporation in GaN?
  • RQ2What are the relative Mn sticking coefficients under Ga-rich, N-rich, and no-flux growth conditions?
  • RQ3Does Mn incorporation correlate with surface morphology changes or polarity-related effects?
  • RQ4Is Mn desorption significant during growth, influencing apparent Mn thicknesses?
  • RQ5How do Mn incorporation trends compare to other dopants like Mg in GaN under similar conditions?

Key findings

  • Mn incorporation is highest under N-rich conditions, about 1×10^20 cm^-3.
  • Mn incorporation is lowest under Ga-rich conditions, about 1×10^18 cm^-3.
  • Mn incorporation under no-flux Mn δ-doping is intermediate, with Mn density around 1×10^19 cm^-3.
  • Relative Mn sticking coefficients (normalized to N-rich) are 0.31 for no-flux and 0.01 for Ga-rich growth.
Figure 2: SIMS depth profiles of GaN:Mn/GaN multilayers grown on a GaN template at 680 ∘ C by MBE, showing (a) O, C, Si, and H and (b) Mn concentrations in the layers, with detection limits of $3\times 10^{15}$ cm -3 for Si and O, $1.5\times 10^{15}$ cm -3 for C, $1\times 10^{17}$ cm -3 for H, and $
Figure 2: SIMS depth profiles of GaN:Mn/GaN multilayers grown on a GaN template at 680 ∘ C by MBE, showing (a) O, C, Si, and H and (b) Mn concentrations in the layers, with detection limits of $3\times 10^{15}$ cm -3 for Si and O, $1.5\times 10^{15}$ cm -3 for C, $1\times 10^{17}$ cm -3 for H, and $

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.