Skip to main content
QUICK REVIEW

[Paper Review] Fabrication and properties of L-arginine-doped PCL electrospun composite scaffolds

Semen Goreninskii, Evgeny Bolbasov|arXiv (Cornell University)|Aug 9, 2017
Electrospun Nanofibers in Biomedical ApplicationsMaterials Science14 references11 citations
TL;DR

This study develops L-arginine-doped poly(ε-caprolactone) (PCL) electrospun scaffolds using hexafluoro-2-propanol as a common solvent, demonstrating that increasing L-arginine content (0.5–1 wt.%) enhances fiber strength and Young's modulus while improving mesenchymal stem cell adhesion and viability. The scaffolds maintain consistent porosity and water contact angle, with optimal biological performance at 0.5–1% L-arginine.

ABSTRACT

The article describes fabrication and properties of composite fibrous scaffolds obtained by electrospinning of the solution of poly({\epsilon}-caprolactone) and arginine in common solvent. The influence of arginine content on structure, mechanical, surface and biological properties of the scaffolds was investigated. It was found that with an increase of arginine concentration diameter of the scaffold fibers was reduced, which was accompanied by an increase of scaffold strength and Young modulus. It was demonstrated that porosity and water contact angle of the scaffold are independent from arginine content. The best cell adhesion and viability was shown on scaffolds with arginine concentration from 0.5 to 1 % wt.

Motivation & Objective

  • To develop biodegradable, L-arginine-doped PCL composite scaffolds for cardiovascular tissue engineering.
  • To overcome the limitation of incompatible solvents for PCL and L-arginine by using hexafluoro-2-propanol as a common solvent.
  • To investigate the influence of L-arginine concentration on the structural, mechanical, surface, and biological properties of electrospun PCL scaffolds.
  • To identify the optimal L-arginine concentration that enhances cell adhesion and viability without compromising scaffold integrity.
  • To establish a scalable method for fabricating functionalized, bioactive PCL-based fibrous scaffolds with sustained nitric oxide release potential.

Proposed method

  • Electrospun PCL/L-arginine composite scaffolds were fabricated using a NANON-01 system at 20 kV voltage, 2 mL/h feed rate, and 150 mm tip-to-collector distance.
  • Hexafluoro-2-propanol was used as a common solvent to dissolve both PCL (Mw = 80 kDa) and L-arginine (≥99%) at concentrations of 0, 0.1, 0.5, 1, 3, and 7 wt.%
  • Fiber morphology and diameter distribution were analyzed via scanning electron microscopy (SEM) and ImageJ software.
  • Surface wettability was assessed using the water contact angle via the sitting drop method (EasyDrop, Kruss).
  • L-arginine presence on the surface was confirmed using 1% ninhydrin solution in ethanol, with thermal behavior analyzed via DSC (20–120 °C).
  • Mechanical properties (Young’s modulus, tensile strength, elongation) were measured via uniaxial tensile testing (Instron 3369) at 10 mm/min strain rate.
  • Porosity was measured using the liquid intrusion method, and crystallinity was calculated using the formula: Xc = (∆Hm / ∆Hm⁰) × 100%, with ∆Hm⁰ = 135.5 J/g for 100% crystalline PCL.
  • Biological evaluation included MMSC adhesion and viability assays, with statistical analysis performed using non-parametric Kruskal-Wallis and Mann-Whitney U tests (p < 0.05).

Experimental results

Research questions

  • RQ1How does increasing L-arginine concentration in PCL electrospinning solutions affect fiber diameter and morphology?
  • RQ2What is the effect of L-arginine doping on the mechanical properties (Young’s modulus, tensile strength, elongation) of PCL scaffolds?
  • RQ3How does L-arginine content influence scaffold porosity and surface wettability (water contact angle)?
  • RQ4What is the optimal L-arginine concentration that maximizes mesenchymal stem cell adhesion and viability on PCL scaffolds?
  • RQ5How does L-arginine incorporation affect the thermal behavior and crystallinity of the composite scaffolds?

Key findings

  • Increasing L-arginine concentration from 0% to 7% wt. reduced average fiber diameter and shifted the fiber diameter distribution from bimodal to unimodal.
  • The Young’s modulus of the scaffolds increased significantly with L-arginine doping, reaching 34 ± 3 MPa at 7% arginine, a 83% increase compared to 18 ± 3 MPa for pure PCL.
  • Maximum tensile strength (14 ± 1 MPa) was observed at 1% L-arginine, while elongation was highest at 7% (176 ± 23%), indicating enhanced ductility at high doping levels.
  • Scaffold porosity and water contact angle remained largely unchanged across all L-arginine concentrations, indicating no significant alteration in surface energy or scaffold architecture.
  • The highest number of adhered mesenchymal stem cells (107 ± 32 cells/mm²) and improved viability (71.6 ± 2.3%) were observed at 0.5% L-arginine, with a significant increase in adhesion compared to pure PCL (52 ± 16 cells/mm²).
  • At 7% L-arginine, viability dropped to 50.0 ± 7.7%, with increased apoptosis (27.6 ± 4.5%), indicating cytotoxicity at high concentrations, thus confirming 0.5–1% as the optimal range.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.