[Paper Review] Revisiting stress-corrosion cracking and hydrogen embrittlement in 7xxx-Al alloys at the near-atomic-scale
This study investigates stress-corrosion cracking (SCC) and hydrogen embrittlement (HE) in 7xxx Al-alloys at the near-atomic scale using transmission electron microscopy (TEM) and atom probe tomography (APT). It reveals hydrogen segregation to dislocation arrays and grain boundaries, formation of a Mg-rich, H-rich amorphous oxide at the crack tip, and oxygen enrichment (>1 at%) in the matrix near the oxide, indicating solute redistribution and localized dealloying that may accelerate crack propagation.
The high-strength 7xxx series aluminium alloys can fulfil the need for light, high strength materials necessary to reduce carbon-emissions, and are extensively used in aerospace for weight reduction purposes. However, as all major high-strength materials, these alloys can be sensitive to stress-corrosion cracking (SCC) through anodic dissolution and hydrogen embrittlement (HE). Here, we study at the near-atomic-scale the intra- and inter-granular microstructure ahead and in the wake of a propagating SCC crack. Moving away from model alloys and non-industry standard tests, we perform a double cantilever beam (DCB) crack growth test on an engineering 7xxx Al-alloy. H is found segregated to planar arrays of dislocations and to grain boundaries that we can associate to the combined effects of hydrogen-enhanced localised plasticity (HELP) and hydrogen-enhanced decohesion (HEDE) mechanisms. We report on a Mg-rich amorphous hydroxide on the corroded crack surface and evidence of Mg-related diffusional processes leading to dissolution of the strengthening η-phase precipitates ahead of the crack.
Motivation & Objective
- To understand the mechanistic role of hydrogen embrittlement and stress-corrosion cracking in high-strength 7xxx Al-alloys under real engineering conditions.
- To resolve the interplay between structural defects (dislocations, grain boundaries), hydrogen, and solute transport during SCC.
- To identify microchemical and microstructural changes ahead of and at the crack tip that influence crack propagation resistance.
- To address the lack of spatially resolved compositional data in SCC studies, particularly regarding hydrogen and oxygen distribution.
- To provide insights into how microstructure evolution and solute redistribution affect service life prediction and material design.
Proposed method
- Performed an industry-standard double cantilever beam (DCB) test on commercial 7449-T7651 7xxx Al-alloy under ambient air to induce intergranular SCC.
- Used site-specific focused ion beam (FIB) milling to prepare TEM and APT specimens from the crack tip and grain boundary regions.
- Conducted atom probe tomography (APT) in voltage-pulsing mode at 75 K with 20% pulse fraction and 125 kHz pulsing rate to achieve near-atomic resolution chemical mapping.
- Employed transmission electron microscopy (TEM) and electron backscatter diffraction (EBSD) to analyze dislocation structures and crack morphology.
- Performed energy-dispersive X-ray spectroscopy (EDS) and selected area electron diffraction (SAED) to confirm the amorphous nature of the oxide layer.
- Calibrated APT reconstructions using established procedures and validated H and O measurements against reference datasets from matrix regions.
Experimental results
Research questions
- RQ1How does hydrogen distribute at the near-atomic scale ahead of and within a propagating SCC crack in 7xxx Al-alloys?
- RQ2What is the chemical and structural nature of the oxide layer formed at the crack tip during SCC in ambient air?
- RQ3How do solute elements (Mg, Zn, Cu, O) redistribute during crack propagation, and what role do dislocations and grain boundaries play in this process?
- RQ4To what extent do microstructural features such as precipitates and grain boundaries influence hydrogen trapping and crack propagation mechanisms?
- RQ5Does localized dealloying and oxygen enrichment in the matrix near the oxide interface contribute to weakening and crack growth?
Key findings
- Hydrogen is found segregated to planar arrays of dislocations and grain boundaries, consistent with hydrogen-enhanced localized plasticity (HELP) and hydrogen-enhanced decohesion (HEDE) mechanisms.
- A Mg-rich, H-rich, non-stoichiometric amorphous oxide forms at the crack tip, with a composition distinct from the bulk alloy and enriched in chlorinated species.
- Oxygen concentration in the matrix near the oxide-metal interface reaches up to 1 at%, significantly exceeding the solubility limit in aluminum, indicating non-equilibrium solute incorporation.
- No measurable increase in hydrogen concentration is observed in the matrix away from the crack, suggesting hydrogen is primarily localized at defects and interfaces.
- Mg and Zn levels in η-phase precipitates ahead of the crack show a linear correlation, indicating compositional changes due to localized dissolution and solute transport.
- Dislocations and grain boundaries act as fast diffusion pathways for solutes, facilitating the localized dealloying of strengthening precipitates and altering the local resistance to crack propagation.