[Paper Review] Temperature-Dependent Dielectric Function of Tantalum Nitride Formed by Atomic Layer Deposition for Tunnel Barriers in Josephson Junctions
The paper measures and models the dielectric function of insulating ALD TaN films across temperatures to assess their suitability as tunnel barriers in Ta-based Josephson junctions, showing insulating behavior and developing a Tauc-Lorentz based dispersion model.
We report the dielectric functions of insulating tantalum nitride (TaN) films, deposited using atomic layer deposition (ALD) on 300 mm Si/SiO2 substrates, to demonstrate their suitability as tunnel barriers in tantalum-based Josephson junctions (JJ) for superconducting quantum circuits. The temperature-dependent ellipsometric angles were measured using ALD TaN films with nominal thicknesses of 13 nm and 25 nm at an incidence angle of 70 degrees, across photon energy ranges of 0.03 eV to 0.7 eV (80-300 K) and 0.5 eV to 6.5 eV (80-600 K). This data was used to develop a dispersion model for insulating ALD TaN films that incorporates a Tauc-Lorentz oscillator with a band gap of 1.5-1.8 eV to model the interband optical transitions. The extracted dielectric function of ALD TaN films shows an insulating behavior (mid-infrared transparency) at all temperatures and for both film thicknesses tested. ALD TaN does not exhibit infrared absorption due to free carriers, even at elevated temperatures, demonstrating its insulating nature, which is required for the tunnel barrier of the JJ in quantum applications. The results of transmission electron microscopy, including selected area electron diffraction, and X-ray diffraction are also discussed. Sputter depth-profile X-ray photoelectron spectroscopy (XPS) shows an N/Ta ratio of ~1.2 throughout the film. The lower band gap, low roughness, and thermal stability of ALD TaN compared to AlOx suggest the possibility of fabricating JJs with thicker barriers while achieving critical current densities required for qubits, better control of thickness and composition, reduced topography, and resistance to aging.
Motivation & Objective
- Demonstrate the insulating dielectric behavior of ALD TaN films for tunnel barrier use in Josephson junctions across 80–600 K.
- Characterize the temperature-dependent optical constants and dispersion of ALD TaN films to enable accurate barrier modeling.
- Develop a dielectric function model incorporating a Tauc-Lorentz oscillator with a specified band gap range (1.5–1.8 eV) for interband transitions.
- Assess the potential advantages of ALD TaN over AlOx in terms of thickness control, roughness, thermal stability, and resistance to aging for qubit applications.
- Correlate structural/compositional analyses with optical properties to support material suitability for superconducting quantum circuits.
Proposed method
- Measure temperature-dependent ellipsometric angles for TaN films (thicknesses 13 nm and 25 nm) on Si/SiO2 at 70° incidence.
- Fit a dispersion model using a Tauc-Lorentz oscillator with a 1.5–1.8 eV band gap to describe interband transitions.
- Assess insulating behavior via mid-infrared transparency and absence of infrared free-carrier absorption up to elevated temperatures.
- Provide supporting structural data from TEM (including selected area diffraction) and XRD, and compositional data from sputter depth-profile XPS (N/Ta ≈ 1.2).
- Compare ALD TaN’s properties with AlOx to discuss implications for thicker barriers and qubit-critical current densities.
Experimental results
Research questions
- RQ1What is the temperature dependence of the dielectric function of insulating ALD TaN films?
- RQ2Can ALD TaN serve as a suitable tunnel barrier material for Ta-based Josephson junctions by maintaining insulating behavior across relevant temperatures?
- RQ3How well does a Tauc-Lorentz-based dispersion model describe the optical transitions in ALD TaN, and what band gap is appropriate?
- RQ4What are the structural and compositional characteristics of ALD TaN films that correlate with their dielectric properties and thermal stability?
Key findings
- ALD TaN films exhibit insulating behavior with mid-infrared transparency across all tested temperatures and thicknesses (13 nm and 25 nm).
- Infrared absorption due to free carriers is not observed, even at elevated temperatures, supporting suitability as tunnel barriers.
- The dispersion model incorporating a Tauc-Lorentz oscillator with a band gap of 1.5–1.8 eV adequately describes interband transitions.
- THIN TaN films show low roughness and thermal stability, suggesting potential for thicker barriers while achieving required critical current densities.
- Sputter depth-profile XPS indicates an N/Ta ratio of approximately 1.2 throughout the film, consistent with measured optical behavior.
- TEM (including selected area diffraction) and XRD analyses are discussed to corroborate the structural nature of the TaN films.
Read this paper