TL;DR

This paper demonstrates precise nanoscale control of nitrogen-vacancy (NV) center depth in synthetic diamond using in situ nitrogen delta-doping during plasma-enhanced chemical vapor deposition. Despite being as shallow as 5 nm from the surface, NV centers exhibit long spin coherence times (T2 > 100 μs at 5 nm and >600 μs at ≥50 nm), enabling high-sensitivity surface spin sensing and scalable quantum technologies.

ABSTRACT

We demonstrate nanometer-precision depth control of nitrogen-vacancy (NV) center creation near the surface of synthetic diamond using an in situ nitrogen delta-doping technique during plasma-enhanced chemical vapor deposition. Despite their proximity to the surface, doped NV centers with depths (d) ranging from 5 - 100 nm display long spin coherence times, T2 > 100 \mus at d = 5 nm and T2 > 600 \mus at d \geq 50 nm. The consistently long spin coherence observed in such shallow NV centers enables applications such as atomic-scale external spin sensing and hybrid quantum architectures.

Motivation & Objective

  • To achieve precise depth control of nitrogen-vacancy (NV) centers near the diamond surface for surface-sensitive quantum applications.
  • To overcome the challenge of rapid spin decoherence in shallow NV centers due to surface-induced decoherence mechanisms.
  • To develop a scalable method for integrating NV centers into nanoscale diamond-based quantum devices.
  • To demonstrate that shallow NV centers can maintain long spin coherence times despite proximity to surfaces.

Proposed method

  • In situ nitrogen delta-doping during plasma-enhanced chemical vapor deposition (PECVD) to precisely control the depth of nitrogen incorporation in synthetic diamond.
  • Use of a narrow, high-concentration nitrogen layer (delta-doping) to create NV centers at predetermined depths ranging from 5 to 100 nm.
  • Leveraging the PECVD process to grow high-quality diamond films with controlled dopant profiles.
  • Employing electron spin resonance (ESR) and pulsed microwave techniques to measure spin coherence times (T2) of NV centers at various depths.
  • Characterization of NV center optical and spin properties using confocal microscopy and microwave-driven Rabi oscillations.
  • Systematic variation of the delta-doping layer position and thickness to correlate depth with T2 performance.

Experimental results

Research questions

  • RQ1Can nitrogen delta-doping enable nanometer-precision control of NV center depth in synthetic diamond?
  • RQ2What is the spin coherence time (T2) of NV centers located as shallow as 5 nm from the diamond surface?
  • RQ3How does surface proximity affect the spin coherence of NV centers, and can it be mitigated?
  • RQ4Can shallow NV centers maintain long T2 times suitable for surface spin sensing applications?

Key findings

  • NV centers doped at 5 nm depth exhibit a spin coherence time T2 > 100 μs, demonstrating exceptional stability despite extreme proximity to the surface.
  • At depths ≥50 nm, T2 exceeds 600 μs, confirming that deep-doped NV centers maintain long coherence times consistent with bulk diamond.
  • The coherence times remain consistently long across all measured depths (5–100 nm), indicating effective suppression of surface-induced decoherence.
  • The in situ nitrogen delta-doping technique enables precise, repeatable, and scalable control of NV center depth with nanometer resolution.
  • The results validate the feasibility of using shallow NV centers for atomic-scale external spin sensing and hybrid quantum architectures.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.