Chunyang Jiang, Xin Zhang|arXiv (Cornell University)|Jun 2, 2017
Advanced Measurement and Detection MethodsEngineering4 citations
TL;DR

This study evaluates system compliance in tensile testing of carbon nanotube (CNT) fibers using two testing machines—Keysight T150 and Instron 3365—demonstrating that the T150’s negligible compliance enables more accurate modulus and strength measurements. By analyzing data dispersion via Weibull statistics, the authors recommend a minimum gauge length of 10 mm to reduce variability and ensure reliable, statistically robust mechanical property assessment for CNT fibers.

ABSTRACT

System compliances of two testing machines (Keysight T150 and Instron 3365) were studied for the tensile testing of carbon nanotube (CNT) fibers. Due to the different gripping methods, the T150's system compliance was nearly zero, while that of the Instron was nonnegligible. By analyzing the data dispersion with the Weibull theory, a safe gauge length of >10 mm was suggested for CNT fibers. Therefore, a standard test procedure should involve the compliance evaluation, choice of gauge length, and Weibull statistical analysis.

Motivation & Objective

  • Address the lack of standardized testing procedures for carbon nanotube (CNT) fibers due to their unique mechanical behavior and ultrafine diameter.
  • Investigate how system compliance in tensile testing machines affects the accuracy of measured modulus and strength in CNT fibers.
  • Assess the impact of gauge length on data dispersion and statistical reliability of mechanical properties in CNT fibers.
  • Propose a standardized test procedure incorporating system compliance evaluation, optimal gauge length selection, and Weibull statistical analysis for CNT fibers.

Proposed method

  • Measured system compliance of two testing machines (Keysight T150 and Instron 3365) using a reference specimen with known modulus.
  • Conducted tensile tests on three types of CNT fibers and one carbon fiber across varying gauge lengths (6–40 mm) to assess deformation and compliance effects.
  • Applied Weibull statistical analysis to fiber strength data using the equation $ P(\sigma) = \exp\left[-\left(\frac{\sigma}{\sigma_0}\right)^m\right] $, where $ \sigma_0 $ is the characteristic strength and $ m $ is the Weibull modulus.
  • Used the estimator $ P(\sigma)_i = 1 - \frac{i}{N+1} $ to rank strength data for Weibull fitting, enabling calculation of $ m $ and $ \sigma_0 $ via linear regression on $ \ln\ln\left[\frac{N+1}{N+1-i}\right] = m\ln(\sigma) - m\ln(\sigma_0) $.
  • Evaluated data dispersion by comparing standard deviation of modulus and strength across different gauge lengths.
  • Used template-gripping with photo paper to minimize fiber damage and ensure consistent grip force, particularly for the Instron machine.

Experimental results

Research questions

  • RQ1How does system compliance in tensile testing machines affect the accuracy of modulus and strength measurements in CNT fibers?
  • RQ2What is the optimal gauge length for minimizing data dispersion and ensuring reliable mechanical property assessment in CNT fibers?
  • RQ3To what extent does Weibull statistical analysis improve the reliability of reported tensile strength values for CNT fibers?
  • RQ4How do different gripping methods (e.g., pneumatic vs. rigid) influence system compliance and test outcome variability?
  • RQ5Can a standardized test procedure be developed for CNT fibers that integrates compliance evaluation, gauge length selection, and statistical analysis?

Key findings

  • The Keysight T150 testing machine exhibited nearly zero system compliance due to its rigid grip design, while the Instron 3365 showed nonnegligible compliance due to softer grip mechanisms.
  • System compliance was found to decrease with increasing fiber modulus, particularly in the Keysight T150, indicating a strong dependency on material stiffness.
  • Data dispersion for both Young’s modulus and tensile strength decreased significantly with increasing gauge length, with the most notable reduction observed beyond 10 mm.
  • For CNTF-C fibers, the Weibull modulus increased from 5.115 (at $ L_0 < 20 $ mm) to 6.916 (at $ L_0 > 20 $ mm), indicating reduced strength dispersion at longer gauge lengths.
  • The characteristic strength $ \sigma_0 $ for CNTF-C fibers was 1377 MPa at $ L_0 < 20 $ mm and 1475 MPa at $ L_0 > 20 $ mm, showing improved accuracy with larger gauge lengths.
  • A safe minimum gauge length of >10 mm is recommended to minimize the influence of local defects and reduce data dispersion in CNT fiber tensile testing.

Read this paper