[Paper Review] Field induced magnetic transition and metastability in Co substituted $Mn_{2}Sb$
This study investigates field-induced first-order ferrimagnetic (FRI) to antiferromagnetic (AFM) transitions in Co-doped Mn₂Sb (Mn₁.₈₅Co₀.₁₅Sb), revealing anomalous thermomagnetic irreversibility and glass-like kinetic arrest of the FRI phase at low temperatures. The key finding is that kinetic arrest and supercooling/superheating irreversibility are anti-correlated, enabling reentrant FRI–AFM–FRI transitions with increasing temperature under field annealing, establishing this system as a model for metastable phase dynamics in itinerant magnets.
A detailed investigation of first order ferrimagnetic (FRI) to antiferromagnetic (AFM) transition in Co (15%) doped $Mn_2Sb$ is carried out. These measurements demonstrate anomalous thermomagnetic irreversibility and glass-like frozen FRI phase at low temperatures. The irreversibility arising between the supercooling and superheating spinodals is distinguised in an ingenious way from the irreversibility arising due to kinetic arrest. Field annealing measurements shows reentrant FRI-AFM-FRI transition with increasing temperature. These measurements also show that kinetic arrest band and supercooling band are anitcorrelated i.e regions which are kinetically arrested at higher temperature have lower supercooling temperature and vice versa.
Motivation & Objective
- To investigate the low-temperature behavior of the first-order FRI to AFM transition in Co-doped Mn₂Sb, focusing on anomalous thermomagnetic irreversibility.
- To distinguish between irreversibility due to kinetic arrest of the FRI phase and that arising from supercooling/superheating effects near the transition.
- To explore the tunability of coexisting FRI and AFM phase fractions via magnetic field and thermal history.
- To determine whether the kinetic arrest and supercooling bands are correlated or anti-correlated in the H–T phase space.
- To establish Mn₁.₈₅Co₀.₁₅Sb as a model system for studying metastable phase dynamics analogous to manganites and intermetallics.
Proposed method
- Performed resistivity measurements using a four-probe technique in a cryostat from 3–300 K under magnetic fields up to 8 T, with field applied parallel to current.
- Conducted zero-field cooling (ZFC), field cooling (FC), and field-cooling warming (FCW) protocols to probe thermal and magnetic history dependence.
- Acquired isothermal R–H (resistivity vs. magnetic field) loops at various temperatures to identify virgin curves lying outside the envelope, indicating kinetic arrest.
- Mapped the H–T phase diagram using R–T and R–H data, identifying regions of coexistence and transition boundaries.
- Used field annealing at different fields (H_an) followed by warming to observe de-arrest behavior and reentrant transitions.
- Analyzed free energy diagrams and transition pathways to distinguish between thermodynamic metastability (supercooling) and kinetic arrest.
Experimental results
Research questions
- RQ1What causes the anomalous thermomagnetic irreversibility observed in Co-doped Mn₂Sb at low temperatures?
- RQ2How do kinetic arrest of the FRI phase and supercooling/superheating effects differ in their origin and manifestation?
- RQ3Is there a correlation or anti-correlation between the kinetic arrest band and the supercooling band in the H–T plane?
- RQ4Can reentrant FRI–AFM–FRI transitions be induced by field annealing and thermal cycling?
- RQ5To what extent can the fractions of coexisting FRI and AFM phases be tuned via magnetic field and thermal history?
Key findings
- The system exhibits anomalous thermomagnetic irreversibility at low temperatures, with virgin resistivity curves lying outside the envelope of field-cooled and zero-field-cooled curves, indicating kinetic arrest of the high-temperature FRI phase.
- Kinetic arrest of the FRI phase is confirmed by field annealing at H_an ≥ 4.5 T, where resistivity curves merge at lower temperatures upon warming, indicating de-arrest with decreasing field.
- A clear anti-correlation is observed between the kinetic arrest band and the supercooling band: regions with higher kinetic arrest temperature have lower supercooling temperature, and vice versa.
- Reentrant FRI–AFM–FRI transitions are observed upon warming after field annealing at H_an > 4 T, with the FRI phase reappearing at higher temperatures, confirmed by resistivity measurements in 4 T field.
- The H–T phase diagram reveals a broad hysteretic region that widens at low temperatures, with a shallow maximum in the lower critical field around 40 K, indicating non-monotonic behavior.
- The system shows tunable coexistence of FRI and AFM phases over wide ranges of temperature and magnetic field, with resistivity values at 300 K independent of field, confirming bulk metallic behavior.
Read this paper
Open the full text in the Nubint reader and ask about any passage as you read.
Read this paper on NubintThis review was generated by AI from the original paper. Please check the paper before citing it.