Skip to main content
QUICK REVIEW

[Paper Review] First-principle study of the near-IR luminescence centers in Bi2O3-GeO2 andBi2O3-SiO2 glasses

V. O. Sokolov, В. Г. Плотниченко|arXiv (Cornell University)|Dec 18, 2014
Glass properties and applicationsMaterials Science20 references19 citations
TL;DR

This first-principles study identifies oxygen-deficient bismuth centers as the origin of near-IR luminescence in Bi2O3–GeO2 and Bi2O3–SiO2 glasses. It proposes that =Bi⋯Ge≡ and =Bi⋯Bi= centers are responsible for 1.2–1.3 µm and 1.8–3.0 µm luminescence, respectively, with thermal migration of oxygen vacancies explaining the observed intensity trade-off between these bands.

ABSTRACT

First-principle study of bismuth-related oxygen-deficient centers ($=$Bi$\cdots$Ge$\equiv$, $=$Bi$\cdots$Si$\equiv$, and $=$Bi$\cdots$Bi$=$ oxygen vacancies) in Bi$_2$O$_3$-GeO$_2$, Bi$_2$O$_3$-SiO$_2$, Bi$_2$O$_3$-Al$_2$O$_3$-GeO$_2$, and Bi$_2$O$_3$-Al$_2$O$_3$-SiO$_2$ hosts is performed. A comparison of calculated spectral properties of the centers with the experimental data on luminescence emission and excitation spectra suggests that luminescence in the 1.2-1.3 $μ$m and 1.8-3.0 $μ$m ranges in Bi$_2$O$_3$-GeO$_2$ glasses and crystals is likely caused by $=$Bi$\cdots$Ge$\equiv$ and $=$Bi$\cdots$Bi$=$ centers, respectively, and the luminescence near 1.1 $μ$m in Bi$_2$O$_3$-Al$_2$O$_3$-GeO$_2$ glasses and crystals may be caused by $=$Bi$\cdots$Ge$\equiv$ center with (AlO$_4$)$^-$ center in the second coordination shell of Ge atom.

Motivation & Objective

  • To identify the atomic-scale structure of bismuth-related near-IR luminescence centers in Bi2O3–GeO2 and Bi2O3–SiO2 glasses.
  • To resolve the long-standing ambiguity regarding the origin of luminescence in bismuth-doped chalcogenide and oxide glasses, particularly in the 1.2–1.3 µm and 1.8–3.0 µm ranges.
  • To explain the observed intensity trade-off between 1.2–1.3 µm and 1.8–3.0 µm luminescence bands in annealed Bi2O3–GeO2 glasses via oxygen vacancy migration.
  • To investigate the role of Al2O3 co-doping in modifying the luminescence properties of Bi2O3–GeO2 systems, particularly the emergence of 1.1 µm emission.

Proposed method

  • Employed density functional theory (DFT) calculations to model bismuth-related oxygen-deficient centers (BiODCs) in Bi2O3–GeO2 and Bi2O3–SiO2 hosts.
  • Constructed and optimized defect models including =Bi⋯Ge≡, =Bi⋯Si≡, =Bi⋯Bi=, and ≡Ge–Ge≡ centers with varying coordination environments.
  • Calculated electronic structure, energy levels, spin-orbit splitting, and transition dipole moments to predict luminescence spectra.
  • Analyzed formation and migration energies of oxygen vacancies to assess thermodynamic stability and dynamic behavior under annealing.
  • Simulated the effect of (AlO4)− centers in the second coordination shell of Ge/Si on Bi–Ge/Si bonding and electronic structure.
  • Compared calculated optical transitions with experimental excitation and emission spectra to validate proposed luminescence centers.

Experimental results

Research questions

  • RQ1What atomic-scale defects are responsible for near-IR luminescence in Bi2O3–GeO2 and Bi2O3–SiO2 glasses?
  • RQ2Why does the 1.2–1.3 µm luminescence intensity decrease while 1.8–3.0 µm luminescence increases upon thermal annealing in Bi2O3–GeO2 glasses?
  • RQ3How does the presence of Al2O3 in Bi2O3–GeO2 glasses influence the luminescence properties and the nature of the active centers?
  • RQ4What is the role of oxygen vacancies in stabilizing and modulating the luminescence behavior of bismuth centers?
  • RQ5How do the electronic structures of =Bi⋯Ge≡ and =Bi⋯Bi= centers differ, and why do they emit at distinct near-IR wavelengths?

Key findings

  • The 1.2–1.3 µm luminescence in Bi2O3–GeO2 glasses and crystals is primarily attributed to =Bi⋯Ge≡ centers, with calculated emission at ~1.25 µm matching experimental data.
  • The 1.8–3.0 µm luminescence observed in annealed Bi2O3–GeO2 glasses and crystals is assigned to =Bi⋯Bi= centers, with calculated emission at ~2.0 µm consistent with experiments.
  • Thermal annealing promotes migration of oxygen vacancies, transforming =Bi⋯Ge≡ centers into =Bi⋯Bi= centers, explaining the observed decrease in 1.2–1.3 µm emission and increase in 1.8–3.0 µm emission.
  • The presence of (AlO4)− centers in the second coordination shell of Ge atoms in Bi2O3–Al2O3–GeO2 systems reduces Bi–Ge covalent interaction, shifts the emission to ~1.1 µm, matching experimental observations.
  • Formation energies of oxygen vacancies are -2.7 eV for =Bi⋯Bi=, +0.8 eV for =Bi⋯Ge≡, +0.9 eV for ≡Ge–Ge≡, and +3.1 eV for ≡Si–Si≡, indicating thermodynamic preference for Bi–Bi and Bi–Ge centers.
  • Spin-orbit splitting increases in =Bi⋯Ge≡ and =Bi⋯Si≡ centers when (AlO4)− is present in the second shell, shifting the electronic structure toward that of two-fold coordinated Bi, consistent with shorter-wavelength emission.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.