Skip to main content
QUICK REVIEW

[Paper Review] Growth of ultra thin vanadium dioxide thin films using magnetron sputtering

Fangfang Song, B. E. White|arXiv (Cornell University)|Aug 12, 2016
Transition Metal Oxide NanomaterialsMaterials Science7 citations
TL;DR

This study demonstrates the successful growth of ultra-thin (42 nm) vanadium dioxide (VO2) films on amorphous SiO2 substrates via reactive DC magnetron sputtering, followed by post-deposition annealing in low-oxygen partial pressure. The films exhibit a resistivity change of over 200× at a metal-insulator transition temperature near 72°C, with a hysteresis width of ~8°C and thermally activated behavior in the insulating phase (activation energy 0.16±0.03 eV), while experiencing significant tensile stress (~2.0 GPa), which shifts the transition temperature by ~4°C.

ABSTRACT

In this work, the results of fabricating ultra thin VO$_2$ films on the technologically relevant amorphous SiO$_2$ surface using reactive DC magnetron sputtering are presented. Results indicate that a post deposition anneal in low partial pressures of oxygen is an effective way at stabilizing the VO$_2$(M$_{1}$) phase on the SiO$_2$ surface. VO$_2$ films with a thickness of 42nm show a continuous microstructure, and undergo a resistivity change of more than a factor of 200 as the temperature of the film increases above 72$^{o}C$. The film shows hysteresis in the metal-insulator transition temperature upon heating and cooling with a width of approximately 8$^o$C. The resistivity of the low temperature semiconducting phase is found to be thermally activated with an activation energy 0.16$\pm$0.03 $ev$. Stress measurements using X-ray diffraction indicate that the ultra thin VO$_2$ film has a large tensile stress of 2.0$\pm$0.2 $GPa$. This value agrees well with the calculated thermal stress due to differential thermal expansion between the VO$_2$ thin film and silicon substrate. The stress leads to a shift of the metal-insulator transition temperature by approximately 4$^{o}C$.

Motivation & Objective

  • To develop a scalable method for growing high-quality ultra-thin VO2 films on technologically relevant amorphous SiO2 substrates.
  • To stabilize the VO2(M1) phase in films below 100 nm thickness, which is challenging due to phase instability and poor crystallinity.
  • To investigate the influence of oxygen partial pressure and post-annealing on phase purity, microstructure, and metal-insulator transition (MIT) characteristics.
  • To quantify residual stress and its impact on the MIT temperature in ultra-thin VO2 films.
  • To enable integration of VO2-based devices into existing silicon-based technologies by demonstrating compatibility with amorphous SiO2.

Proposed method

  • Reactive DC magnetron sputtering of vanadium metal target on thermally oxidized Si substrates at 550°C with controlled O2/Ar gas flow ratios (1.9–3 sccm) to tune oxygen partial pressure.
  • Post-deposition annealing in low-oxygen partial pressures (0–4.8×10⁻² Pa) at 550°C to stabilize the VO2(M1) phase.
  • Use of Glancing Incidence X-ray Diffraction (GIXRD) to identify crystallographic phases and assess phase purity.
  • X-ray reflectivity for precise thickness measurement of the ultra-thin films.
  • X-ray diffraction-based residual stress measurements to quantify tensile stress in the films.
  • Electrical characterization using a Keithley 4200 semiconductor parameter analyzer to measure resistivity and MIT behavior across temperature cycles.

Experimental results

Research questions

  • RQ1Can ultra-thin VO2 films (≤100 nm) be stabilized in the desired VO2(M1) phase on amorphous SiO2 using reactive sputtering and post-annealing?
  • RQ2How does oxygen partial pressure during sputtering affect the phase composition and crystallinity of VO2 films?
  • RQ3What is the electrical response (resistivity change, hysteresis width, activation energy) of ultra-thin VO2 films near the metal-insulator transition?
  • RQ4To what extent does intrinsic stress in ultra-thin VO2 films shift the MIT temperature?
  • RQ5Can the MIT be preserved in films as thin as 42 nm while maintaining high resistivity contrast?

Key findings

  • Ultra-thin VO2 films of 42 nm thickness exhibit a resistivity change of over 200× across the metal-insulator transition at ~72°C.
  • The metal-insulator transition shows hysteresis of approximately 8°C during heating and cooling cycles.
  • The low-temperature semiconducting phase exhibits thermally activated resistivity with an activation energy of 0.16±0.03 eV.
  • The film experiences a large tensile stress of 2.0±0.2 GPa, which is consistent with thermally induced stress from the mismatch in thermal expansion coefficients between VO2 and the Si substrate.
  • This stress induces a shift of the MIT temperature by approximately 4°C, demonstrating the significant impact of strain on phase transition behavior.
  • Post-deposition annealing in low-oxygen partial pressure is critical for stabilizing the VO2(M1) phase and achieving high-quality, phase-pure films on amorphous SiO2.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.