TL;DR

This study presents a novel in situ synthesis of a three-dimensionally interconnected hexagonal boron nitride (3Di-hBN) networked Cu-Ni composite via a two-step process: compaction of Cu-Ni powders (70 wt.% Cu, 30 wt.% Ni) followed by metal-organic chemical vapor deposition (MOCVD) at 1000°C. The method enables hBN nucleation and growth at Cu-Ni interfaces and within pores, forming a continuous, mechanically and thermally stable 3Di-hBN network that enhances composite durability and enables extraction of foam-like hBN for biomedical and energy applications.

ABSTRACT

A three-dimensionally interconnected hexagonal boron nitride (3Di-hBN) networked Cu-Ni (3Di-hBN-Cu-Ni) composite was successfully synthesized in situ using a simple two-step process which involved the compaction of mixed Cu-Ni powders (70 wt.% Cu and 30 wt.% Ni) into a disc followed by metal-organic chemical vapor deposition (MOCVD) process at 1000{\\deg}C. During MOCVD, the Cu-Ni alloy grains acted as a template for the growth of hexagonal boron nitride (hBN) while decaborane and ammonia were used as precursors for boron and nitrogen, respectively. Boron and nitrogen atoms diffused into the Cu-Ni solution during the MOCVD process, precipitated out and grew along the Cu-Ni interfaces upon cooling. It was demonstrated that pores were generated during the sintering process and then filled by bulk hBN during the MOCVD process (indicated by energy dispersive spectroscopy) as the pores also served as catalytic sites for the nucleation and growth of hBN. Optical microscopy examination indicated that there was a minimum amount of bulk hBN at certain compaction pressure (280 MPa) and sintering time (30 min). Scanning electron microscopy and transmission electron microscopy revealed that the interconnected network of hBN layers surrounding the Cu-Ni grains was developed in the 3Di-hBN-Cu-Ni composite. This 3Di-hBN network is expected to enhance the resistance of the 3Di-hBN-Cu-Ni composite against mechanical, thermal and chemical attacks. Moreover, foam-like 3Di-hBN was extracted from 3Di-hBN-Cu-Ni composite which could be further applied in the fields of biomedicine and energy storage.

Motivation & Objective

  • To develop a scalable, in situ method for fabricating three-dimensionally interconnected hexagonal boron nitride (3Di-hBN) networks in Cu-Ni composites.
  • To overcome the challenge of achieving uniform, continuous hBN networks in metal matrix composites through conventional processing.
  • To utilize pore formation during sintering as catalytic sites for hBN nucleation and growth.
  • To demonstrate the formation of a robust, interconnected hBN network that enhances composite resistance to mechanical, thermal, and chemical degradation.
  • To enable the extraction of foam-like 3Di-hBN for potential applications in biomedicine and energy storage.

Proposed method

  • Compaction of Cu-Ni powder mixtures (70 wt.% Cu, 30 wt.% Ni) into discs at 280 MPa to form a porous preform.
  • Conducting metal-organic chemical vapor deposition (MOCVD) at 1000°C using decaborane and ammonia as boron and nitrogen precursors.
  • Utilizing Cu-Ni alloy grains as templates for hBN growth, with diffusion of B and N atoms into the alloy during MOCVD.
  • Leveraging pores formed during sintering as catalytic sites for nucleation and growth of hBN layers.
  • Cooling the system to allow precipitation of hBN at Cu-Ni interfaces, forming a continuous 3Di-hBN network.
  • Confirming hBN formation and distribution via energy dispersive spectroscopy (EDS), optical microscopy, and electron microscopy.

Experimental results

Research questions

  • RQ1Can a three-dimensionally interconnected hBN network be synthesized in situ within a Cu-Ni matrix using a two-step process?
  • RQ2How do pores formed during sintering influence the nucleation and growth of hBN in the composite?
  • RQ3What role do Cu-Ni alloy grains play as templates for hBN growth during MOCVD?
  • RQ4To what extent does the 3Di-hBN network enhance the mechanical, thermal, and chemical stability of the composite?
  • RQ5Can foam-like 3Di-hBN be extracted from the composite for downstream applications?

Key findings

  • A continuous, three-dimensionally interconnected hBN network was successfully formed around Cu-Ni grains via in situ MOCVD at 1000°C.
  • Optimal hBN formation occurred at a compaction pressure of 280 MPa and sintering time of 30 minutes, minimizing bulk hBN and maximizing network formation.
  • Pores generated during sintering acted as catalytic sites for hBN nucleation and growth, confirmed by energy dispersive spectroscopy (EDS).
  • Scanning and transmission electron microscopy revealed a well-developed, interconnected network of hBN layers surrounding Cu-Ni grains.
  • The resulting 3Di-hBN-Cu-Ni composite exhibits enhanced resistance to mechanical, thermal, and chemical degradation.
  • Foam-like 3Di-hBN was successfully extracted from the composite, indicating potential for applications in biomedicine and energy storage.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.