[Paper Review] Atomic layer deposition of titanium nitride for quantum circuits
This paper demonstrates atomic layer deposition (ALD)-grown titanium nitride (TiN) thin films for high kinetic inductance microwave resonators, achieving internal quality factors exceeding 1 million at single-photon power and characteristic impedances up to 28 kΩ. The high-impedance resonators, fabricated using a capacitor-free meandered inductor design, enable a 24-fold enhancement in single-photon coupling strength, making them ideal for hybrid quantum systems and quantum sensing applications.
Superconducting thin films with high intrinsic kinetic inductance are of great importance for photon detectors, achieving strong coupling in hybrid systems, and protected qubits. We report on the performance of titanium nitride resonators, patterned on thin films (9-110 nm) grown by atomic layer deposition, with sheet inductances of up to 234 pH/square. For films thicker than 14 nm, quality factors measured in the quantum regime range from 0.4 to 1.0 million and are likely limited by dielectric two-level systems. Additionally, we show characteristic impedances up to 28 kOhm, with no significant degradation of the internal quality factor as the impedance increases. These high impedances correspond to an increased single photon coupling strength of 24 times compared to a 50 Ohm resonator, transformative for hybrid quantum systems and quantum sensing.
Motivation & Objective
- To develop wafer-scale, uniform superconducting thin films with high kinetic inductance for quantum circuit applications.
- To overcome limitations of conventional deposition methods by using atomic layer deposition (ALD) for consistent, conformal TiN film growth.
- To achieve high characteristic impedance in microwave resonators without sacrificing internal quality factor (Qi).
- To enable enhanced spin-photon coupling in hybrid quantum systems through increased zero-point electric field fluctuations.
- To explore the performance limits of ultra-thin ALD-TiN films in high-impedance resonator architectures.
Proposed method
- Atomic layer deposition (ALD) at 270 °C on hydrogen-terminated, high-resistivity Si(111) substrates to grow uniform TiN films (9–110 nm thick).
- Use of a lumped-element resonator design with a meandered inductor wire (no explicit capacitor) to maximize characteristic impedance while minimizing stray capacitance.
- Measurement of sheet inductance (L□) and critical temperature (Tc) via DC electrical characterization to assess superconducting properties.
- X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) to confirm film crystallinity and stoichiometry.
- Resonator performance evaluated at 20 mK using microwave reflection measurements to extract internal quality factor (Qi) and resonance frequency.
- Characteristic impedance (Z) calculated from f0, L□, wire width (w), and length (ℓ) using Z ∝ (ℓ/w³)¹ᐟ⁴, with experimental calibration.
Experimental results
Research questions
- RQ1Can ALD-grown TiN films achieve high kinetic inductance and superconducting coherence suitable for quantum circuits?
- RQ2How does film thickness affect the internal quality factor (Qi) of ALD-TiN resonators at single-photon power levels?
- RQ3To what extent can characteristic impedance be increased in ALD-TiN resonators without degrading Qi?
- RQ4What limits the internal quality factor—dielectric two-level systems or suppressed superconductivity in thin films?
- RQ5Can ultra-thin ALD-TiN films support high-impedance resonators with minimal loss for enhanced spin-photon coupling?
Key findings
- ALD-grown TiN films with thickness ≥14.2 nm achieve internal quality factors (Qi) of 0.4–1.0 million at single-photon power, indicating high coherence.
- The thinnest film (8.9 nm) achieves a characteristic impedance of 28 kΩ, corresponding to a 24-fold increase in single-photon coupling strength compared to 50 Ω resonators.
- No significant degradation in Qi is observed as impedance increases, even at wire widths as narrow as 75 nm, demonstrating robust performance across high-impedance designs.
- Sheet inductance reaches up to 234 pH/□ in thicker films, confirming high kinetic inductance from the large London penetration depth.
- For the thinnest film, Qi ≈ 1×10⁵ is observed despite deviations from BCS theory, suggesting suppression of superconductivity as a dominant loss mechanism.
- The absence of strong Qi dependence on wire width down to 75 nm indicates that the design effectively decouples impedance scaling from coherence loss.
Read this paper
Open the full text in the Nubint reader and ask about any passage as you read.
Read this paper on NubintThis review was generated by AI from the original paper. Please check the paper before citing it.