Skip to main content
QUICK REVIEW

[Paper Review] Substrate effect and nanoindentation fracture toughness based on pile up and failure

A. S. Bhattacharyya, Ramagiri Praveen Kumar|arXiv (Cornell University)|Feb 23, 2016
Metal and Thin Film MechanicsEngineering9 references4 citations
TL;DR

This study investigates the substrate effect on nanoindentation fracture toughness in thin films using Berkovich indenter tests, focusing on pile-up behavior and failure mechanisms. By analyzing load-displacement curves, energy partitioning, and delamination geometry, the authors establish a correlation between substrate-induced dislocation pile-up, tip blunting, and fracture toughness (KR), demonstrating that film thickness and substrate hardness significantly influence measured toughness and failure modes.

ABSTRACT

The effect of substrate was studied using nanoindentation on thin films. Soft films on hard substrate showed more pile up than usual which was attributed to the dislocation pile up at the film substrate interface. The effect of tip blunting on the load depth and hardness plots of nanoindentation was shown. The experimental date of variation of Vickers hardness with film thickness and loads were fitted and new parameters were analyzed. The delaminated area was analyzed using geometrical shapes using optical view of the failure region along with the load displacement Indentation fracture using Nanoindentation using Berkovich indenter has been studied. Indentation fracture toughness (KR) was analyzed based on computational programs. The contact mechanics during nanoindentation was studied with parameters related to indenter shape and tip sharpness. Elastic, plastic and total energies were computationally determined. The energy difference was related to shear stress being generated with elastic to plastic transition. Change in the nature of residual stress was related to film thickness.

Motivation & Objective

  • To understand how substrate properties influence pile-up and fracture behavior during nanoindentation of thin films.
  • To quantify the effect of substrate hardness on dislocation pile-up at the film-substrate interface.
  • To correlate tip blunting with changes in load-depth response and hardness measurements.
  • To develop a computational framework linking residual stress, energy partitioning, and fracture toughness (KR).
  • To analyze delamination area geometry from optical images to assess failure mechanisms in thin film systems.

Proposed method

  • Conducting nanoindentation tests using a Berkovich indenter on thin films deposited on various substrates.
  • Measuring load-displacement curves to extract hardness and elastic/plastic energy contributions.
  • Analyzing optical images of the failure region to determine delamination area using geometric modeling.
  • Computing elastic, plastic, and total energies from the load-displacement data to assess energy dissipation.
  • Using computational models to relate shear stress at the elastic-plastic transition to fracture toughness (KR).
  • Fitting experimental Vickers hardness data with film thickness and load to extract new mechanical parameters.

Experimental results

Research questions

  • RQ1How does substrate hardness influence dislocation pile-up and surface pile-up morphology during nanoindentation?
  • RQ2To what extent does tip blunting affect the measured hardness and load-depth response in thin film systems?
  • RQ3How does film thickness modulate residual stress and failure mode in thin films under nanoindentation?
  • RQ4What is the relationship between energy partitioning (elastic vs. plastic) and fracture toughness (KR) in thin films?
  • RQ5Can geometric analysis of delamination zones provide reliable estimates of fracture toughness in nanoindentation?

Key findings

  • Soft films on hard substrates exhibit enhanced pile-up due to dislocation accumulation at the film-substrate interface.
  • Tip blunting leads to measurable changes in load-depth curves and apparent hardness values, affecting toughness quantification.
  • The measured Vickers hardness varies with film thickness and applied load, and the data were successfully fitted to extract new mechanical parameters.
  • Delamination areas were quantified using geometric modeling of optical images, revealing distinct failure patterns dependent on substrate properties.
  • Computed energy partitioning showed a clear correlation between shear stress at the elastic-to-plastic transition and fracture toughness (KR).
  • Fracture toughness (KR) was found to be significantly influenced by film thickness and substrate-induced residual stresses.

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.