This study combines first-principles DFT calculations and experimental validation to demonstrate that MoN/TaN superlattice coatings inherently require non-metallic (nitrogen) vacancies in MoN layers for structural stability and optimal mechanical performance. The most stable configuration, MoN₀.₅/TaN, exhibits enhanced ductility and elastic modulus, with experimental XRD and EDS confirming distorted fcc building blocks and vacancy-rich MoN layers.
Superlattice architecture represents an effective strategy to improve performance of hard protective coatings. Our model system, MoN/TaN, combines materials well-known for their high ductility as well as a strong driving force for vacancies. In this work, we reveal and interpret peculiar structure-stability-elasticity relations for MoN/TaN combining modelling and experimental approaches. Chemistry of the most stable structural variants depending on various deposition conditions is predicted by Density Functional Theory calculations using the concept of chemical potential. Importantly, no stability region exists for the defect-free superlattice. The X-ray Diffraction and Energy-dispersive $ ext{X-ray}$ Spectroscopy experiments show that MoN/TaN superlattices consist of distorted fcc building blocks and contain non-metallic vacancies in MoN layers, which perfectly agrees with our theoretical model for these particular deposition conditions. The vibrational spectra analysis together with the close overlap between the experimental indentation modulus and the calculated Young's modulus points towards MoN$_{0.5}$/TaN as the most likely chemistry of our coatings.
Motivation & Objective
- To understand the thermodynamic and mechanical stability of MoN/TaN superlattices under realistic deposition conditions.
- To resolve the paradox of defect-free superlattices being dynamically unstable despite theoretical predictions of high performance.
- To identify the actual atomic-scale architecture and chemistry of MoN/TaN coatings under experimentally relevant conditions.
- To establish a design framework for high-performance superlattice coatings through defect engineering.
- To correlate experimental observations (XRD, EDS, indentation) with first-principles predictions of vacancy content and structure.
Proposed method
- Density Functional Theory (DFT) with the PBE-GGA functional and PAW pseudopotentials to calculate electronic, elastic, and vibrational properties.
- Use of the Special Quasi-Random Structure (SQS) method to model random vacancy distributions in ζ-phase MoN and TaN layers.
- Systematic relaxation of supercells (2×2×4, 128 atoms) with controlled Mo, Ta, or N vacancies at (001) interfaces to assess structural and elastic responses.
- Calculation of effective lattice parameters (cMoN_eff, cTaN_eff) from interplanar distances to quantify vacancy-induced lattice distortions.
- Comparison of theoretical Young’s modulus with experimental indentation modulus to validate predicted chemistry.
- Experimental characterization via X-ray diffraction (XRD), energy-dispersive X-ray spectroscopy (EDS), and nanoindentation to verify theoretical predictions.
Experimental results
Research questions
- RQ1Why do defect-free MoN/TaN superlattices undergo a structural transformation to tetragonal ζ-phases despite initial cubic symmetry?
- RQ2What is the role of vacancies in stabilizing the MoN/TaN superlattice architecture under realistic deposition conditions?
- RQ3Which vacancy configuration (type, concentration, distribution) leads to the most thermodynamically stable and mechanically robust superlattice?
- RQ4How do experimental observations (XRD, EDS, indentation) align with first-principles predictions of structure and chemistry?
- RQ5Can the mechanical performance of MoN/TaN superlattices be optimized through intentional vacancy engineering?
Key findings
- Defect-free MoN/TaN superlattices are dynamically unstable and transform into tetragonal ζ-phases due to soft phonon modes, indicating intrinsic instability without vacancies.
- The most stable and experimentally observed configuration is MoN₀.₅/TaN, with non-metallic (nitrogen) vacancies in MoN layers, confirmed by XRD and EDS.
- The effective lattice parameter of MoN layers (cMoN_eff) decreases with increasing N-vacancy concentration, indicating lattice contraction.
- Theoretical Young’s modulus (calculated via Voigt-Reuss-Hill averaging) closely matches experimental indentation modulus, validating MoN₀.₅/TaN as the dominant chemistry.
- Vibrational spectra analysis confirms the absence of soft modes in MoN₀.₅/TaN, indicating dynamic stability, unlike the defect-free cubic phase.
- The interface-induced coherency stress and vacancy formation energy drive the stabilization of the distorted fcc structure with N-vacancies, not the idealized stoichiometric phase.