[Paper Review] Two-dimensional Platinum Diselenide Waveguide-Integrated Infrared Photodetectors

Shayan Parhizkar, Maximilian Prechtl|arXiv (Cornell University)|Oct 17, 2021
Photonic and Optical DevicesEngineering81 references37 citations
TL;DR

This study demonstrates waveguide-integrated infrared photodetectors based on two-dimensional platinum diselenide (PtSe2) grown directly on silicon photonic waveguides via thermally assisted conversion (TAC) at low temperatures (<450 °C). The direct-growth approach yields photodetectors with 11 mA/W responsivity at 1550 nm and sub-8.4 μs response times, outperforming transfer-based devices due to conformal, wrinkle-free integration and superior material quality.

ABSTRACT

Low cost, easily integrable photodetectors (PDs) for silicon (Si) photonics are still a bottleneck for photonic integrated circuits (PICs), especially for wavelengths above 1.8 ${\mu}$m. Multilayered platinum diselenide (PtSe$_2$) is a semi-metallic two-dimensional (2D) material that can be synthesized below 450${\deg}$C. We integrate PtSe$_2$ based PDs directly by conformal growth on Si waveguides. The PDs operate at 1550 nm wavelength with a maximum responsivity of 11 mA/W and response times below 8.4 ${\mu}$s. Fourier transform infrared spectroscopy (FTIR) in the wavelength range from 1.25 ${\mu}$m to 28 ${\mu}$m indicates the suitability of PtSe$_2$ for PDs far into the infrared wavelength range. Our PtSe$_2$ PDs integrated by direct growth outperform PtSe$_2$ PDs manufactured by standard 2D layer transfer. The combination of IR responsivity, chemical stability, selective and conformal growth at low temperatures, and the potential for high carrier mobility, make PtSe$_2$ an attractive 2D material for optoelectronics and PICs.

Motivation & Objective

  • To develop low-temperature, integrable infrared photodetectors for silicon photonic integrated circuits.
  • To overcome limitations of conventional materials by leveraging 2D transition metal dichalcogenides with broadband IR response.
  • To compare direct-growth PtSe2 integration with conventional wet transfer methods for waveguide-integrated photodetectors.
  • To evaluate the performance and material quality of PtSe2-based photodetectors in terms of responsivity, response time, and structural integrity.

Proposed method

  • PtSe2 layers were grown directly on Si waveguides via thermally assisted conversion (TAC) at <450 °C, using pre-patterned sputtered Pt as a precursor.
  • A 10.8 nm Pt layer was converted into a 27 nm thick PtSe2 film, conformally covering waveguide sidewalls.
  • A 90 nm Al2O3 barrier layer was deposited via atomic layer deposition (ALD) to protect Si waveguides and grating couplers during TAC.
  • For comparison, PtSe2 films of 7.6, 13.7, and 23.5 nm thickness were grown on separate SiO2 substrates and wet-transferred onto waveguides.
  • Photodetectors were fabricated with 50 μm wide, 5 μm electrode-spaced channels on waveguides, with electrical and optical characterization performed using lock-in amplifiers and oscilloscopes.
  • Raman spectroscopy and AFM were used to confirm PtSe2 formation and measure thickness, while FTIR spectroscopy confirmed broadband IR response from 1.25 μm to 28 μm.

Experimental results

Research questions

  • RQ1Can direct, low-temperature TAC growth of PtSe2 on Si waveguides enable high-performance, conformal photodetectors for silicon photonics?
  • RQ2How does the performance of directly grown PtSe2 photodetectors compare to those fabricated via wet transfer in terms of responsivity and response time?
  • RQ3What is the broadband infrared response of PtSe2 across the 1.25–28 μm range, and how does it support long-wavelength detection?
  • RQ4To what extent does the direct growth method reduce interfacial defects and strain compared to wet transfer, particularly at waveguide edges?
  • RQ5What is the impact of PtSe2 thickness and crystallinity on device performance, as confirmed by Raman and AFM analysis?

Key findings

  • The direct-growth PtSe2 photodetectors achieved a maximum responsivity of 11 mA/W at 1550 nm, significantly outperforming wet-transfer-based devices.
  • Response times were below 8.4 μs, indicating high-speed operation suitable for high-bandwidth applications.
  • Fourier transform infrared (FTIR) spectroscopy confirmed broadband IR absorption from 1.25 μm to 28 μm, demonstrating suitability for mid- and long-wavelength infrared detection.
  • Raman spectroscopy revealed characteristic Eg (177 cm⁻¹) and A1g (206 cm⁻¹) modes, with peak shifts and intensity ratios indicating multilayered PtSe2 formation.
  • AFM measurements confirmed uniform, conformal PtSe2 coverage on waveguides in the direct-growth samples, with no wrinkles or air gaps, unlike the wet-transfer counterparts.
  • IV measurements showed near-ohmic behavior (linear I-V curves) at low voltages, with deviations at higher voltages indicating Schottky barrier formation at PtSe2/electrode interfaces.

Read this paper