[Paper Review] Unsupervised Welding Defect Detection Using Audio And Video
This paper proposes an unsupervised deep learning approach for real-time robotic welding defect detection using audio and video sensors, leveraging a large industrial dataset of 4,000+ weld samples. The multi-modal method achieves an average AUC of 0.92 across 11 defect types, demonstrating that combining audio and video significantly improves detection performance over single-modal approaches.
In this work we explore the application of AI to robotic welding. Robotic welding is a widely used technology in many industries, but robots currently do not have the capability to detect welding defects which get introduced due to various reasons in the welding process. We describe how deep-learning methods can be applied to detect weld defects in real-time by recording the welding process with microphones and a camera. Our findings are based on a large database with more than 4000 welding samples we collected which covers different weld types, materials and various defect categories. All deep learning models are trained in an unsupervised fashion because the space of possible defects is large and the defects in our data may contain biases. We demonstrate that a reliable real-time detection of most categories of weld defects is feasible both from audio and video, with improvements achieved by combining both modalities. Specifically, the multi-modal approach achieves an average Area-under-ROC-Curve (AUC) of 0.92 over all eleven defect types in our data. We conclude the paper with an analysis of the results by defect type and a discussion of future work.
Motivation & Objective
- To enable real-time, automated detection of welding defects during robotic arc welding to reduce post-weld correction costs.
- To address the challenge of limited labeled defect data by using an unsupervised anomaly detection approach trained only on good weld samples.
- To evaluate the effectiveness of audio and video modalities individually and in combination for defect detection in industrial robotic welding.
- To build a large, diverse, multi-modal dataset of real-world robotic welding samples to support robust model training and evaluation.
- To develop a system that can detect defects early in the process, enabling potential real-time parameter adjustments to prevent failures.
Proposed method
- The authors collected over 4,000 real-world robotic welding samples across various weld types, materials, and defect categories in an industrial environment.
- Audio and video data were recorded simultaneously during the welding process using microphones and cameras, capturing both visual and acoustic signals.
- A deep learning-based unsupervised anomaly detection framework was trained exclusively on normal (defect-free) weld samples to avoid bias toward specific defect patterns.
- The model uses feature extraction from raw audio and video streams, followed by reconstruction or reconstruction-based anomaly scoring to detect deviations.
- Multi-modal fusion was achieved by concatenating embeddings from audio and video encoders, enabling joint analysis and improved detection performance.
- Performance was evaluated using the Area Under the ROC Curve (AUC), with separate metrics computed per defect type and modality.
Experimental results
Research questions
- RQ1Can unsupervised deep learning models detect a wide range of welding defects using only audio and video signals during the welding process?
- RQ2How does the performance of defect detection vary between audio-only, video-only, and multi-modal approaches across different defect types?
- RQ3To what extent does combining audio and video signals improve detection accuracy compared to single-modality methods?
- RQ4How robust is the unsupervised approach to variations in welding parameters, materials, and weld geometry?
- RQ5Can the proposed method detect defects early enough in the process to enable real-time corrective actions in industrial robotic welding?
Key findings
- The multi-modal approach achieved an average AUC of 0.92 across all 11 defect types, demonstrating strong generalization and detection capability.
- Audio-only detection achieved high performance for certain defects like porosity and burnthrough, indicating that acoustic signals are highly informative for specific defect types.
- Video-only detection performed well for defects involving visible geometry changes, such as excessive penetration and lack of fusion, which affect the weld pool appearance.
- The combination of audio and video consistently outperformed single-modality models, with the highest AUCs observed for complex defects like porosity with excessive penetration.
- The unsupervised training strategy generalized well across diverse materials (FE410, BSK46) and weld types (fillet, non-fillet), showing robustness to real-world variations.
- Defect detection performance varied by defect type, with the highest AUCs observed for burnthrough (0.95) and porosity (0.94), while warping and spatter showed lower but still significant detection rates.
Read this paper