[Paper Review] A multimodal operando neutron study of the phase evolution in a graphite electrode
This study presents a novel in-situ multimodal operando neutron approach combining attenuation contrast imaging, diffraction contrast imaging, and neutron diffraction to simultaneously map lithium distribution and phase evolution in a graphite electrode during lithiation and delithiation. The key contribution is the direct correlation of spatially resolved lithium uptake and structural phase transformations, revealing a Li-content gradient during insertion and confirming complete Li extraction during delithiation, with solid electrolyte interphase (SEI) formation contributing more to attenuation than Li insertion overall.
Obtaining a complete picture of local processes still poses a significant challenge in battery research. Here we demonstrate an in-situ combination of multimodal neutron imaging with neutron diffraction for spatially resolved operando observations of the lithiation-delithiation of a graphite electrode in a Li-ion battery cell. Throughout the lithiation-delithiation process we image the Li distribution based on the local beam attenuation. Simultaneously, we observe the development of the lithiated graphite phases as a function of cycling time and electrode thickness and integral throughout its volume by diffraction contrast imaging and diffraction, respectively. While the conventional imaging data allows to observe the Li uptake in graphite already during the formation of the solid electrolyte interphase, diffraction indicates the onset and development of the Li insertion/extraction globally, which supports the local structural transformation observations by diffraction contrast imaging.
Motivation & Objective
- To overcome the challenge of correlating local lithium distribution with crystallographic phase evolution in lithium-ion battery electrodes.
- To address the limitations of conventional imaging and diffraction by combining them in a single in-situ experiment for improved spatial and structural resolution.
- To distinguish between attenuation due to lithium insertion and that due to SEI formation or electrolyte variation.
- To provide a comprehensive, time-resolved view of electrochemical processes across multiple length scales in a model graphite electrode.
- To validate the reliability of attenuation contrast imaging by cross-referencing with diffraction data to exclude artifacts from electrolyte movement or bubble formation.
Proposed method
- Employed a custom-designed half-cell with a graphite anode for operando neutron studies.
- Combined three neutron-based techniques: attenuation contrast imaging (for local Li content), diffraction contrast imaging (for local phase transformation), and bulk neutron diffraction (for global phase evolution).
- Performed in-situ measurements at the J-PARC and Paul Scherrer Institute (PSI) facilities using the SENJU and RADEN beamlines.
- Used wavelength-resolved transmission measurements to extract Bragg edge information for diffraction contrast imaging.
- Correlated attenuation changes with diffraction data to distinguish Li insertion from SEI formation and electrolyte effects.
- Applied data processing techniques to reconstruct 3D Li distribution and phase evolution over time and electrode thickness.
Experimental results
Research questions
- RQ1How does lithium distribution evolve spatially and temporally during lithiation and delithiation in a graphite electrode?
- RQ2To what extent do solid electrolyte interphase (SEI) formation and lithium insertion contribute to neutron beam attenuation?
- RQ3Can diffraction contrast imaging resolve local phase transformations in real time and correlate them with global diffraction data?
- RQ4Is the lithium insertion process homogeneous or gradient-driven across the electrode thickness?
- RQ5What fraction of the initial lithium is successfully extracted during delithiation, and what residual phases remain?
Key findings
- The SEI formation process contributed more to the overall attenuation increase in the graphite electrode than lithium insertion, particularly in regions of low Li concentration.
- Lithium insertion created a distinct gradient in Li content, with higher concentrations near the separator, peaking during the formation of the LiC12 phase.
- The delithiation process was slower and more homogeneous after the lithiation gradient disappeared, indicating complete extraction of inserted Li+ ions.
- Diffraction data confirmed that the fully delithiated state at 55 hours closely resembled the state after full SEI formation at around 12 hours, indicating no significant SEI growth during lithiation.
- Diffraction contrast imaging successfully excluded artifacts from electrolyte movement and bubble formation, providing spatially resolved validation of phase transformation dynamics.
- The combination of imaging and diffraction enabled direct, time-correlated observation of local and global processes, proving superior to sequential or isolated measurements.
Read this paper