Skip to main content
QUICK REVIEW

[Paper Review] Calibration and data analysis routines for nanoindentation with spherical tips

Diana Avadanii, Anna Kareer|arXiv (Cornell University)|Feb 5, 2023
Metal and Thin Film MechanicsEngineering54 references3 citations
TL;DR

This paper presents a validated, integrated calibration and data analysis workflow for spherical nanoindentation using elastic reference materials (fused silica, sapphire, glassy carbon) to independently determine effective tip radius and machine stiffness. By parametrizing the effective radius as a function of load and applying this routine to materials like olivine, titanium, and tungsten, the authors extract accurate indentation stress-strain curves and demonstrate the critical impact of machine stiffness on yield stress identification and indentation size effect assessment.

ABSTRACT

Instrumented spherical nanoindentation with a continuous stiffness measurement has gained increased popularity in material science studies in brittle and ductile materials alike. These investigations span hypotheses related to a wide range of microphysics involving grain boundaries, twins, dislocation densities, ion-induced damage and more. These studies rely on the implementation of different methodologies for instrument calibration and for circumventing tip shape imperfections. In this study, we test, integrate, and re-adapt published strategies for tip and machine-stiffness calibration for spherical tips. We propose a routine for independently calibrating the effective tip radius and the machine stiffness using three reference materials (fused silica, sapphire, glassy carbon), which requires the parametrization of the effective radius as a function of load. We validate our proposed workflow against key benchmarks, such as variation of Young's modulus with depth. We apply the resulting calibrations to data collected in materials with varying ductility (olivine, titanium, and tungsten) to extract indentation stress-strain curves. We also test the impact of the machine stiffness on recently proposed methods for identification of yield stress, and compare the influence of different conventions on assessing the indentation size effect. Finally, we synthesize these analysis routines in a single workflow for use in future studies aiming to extract and process data from spherical nanoindentation.

Motivation & Objective

  • To address inconsistencies in spherical nanoindentation data caused by tip shape imperfections, machine stiffness variations, and calibration errors.
  • To develop a unified, reproducible calibration routine that independently determines effective tip radius and machine stiffness using purely elastic indentation on reference materials.
  • To validate the workflow against benchmarks such as depth-dependent Young’s modulus and indentation size effect.
  • To enable reliable extraction of indentation stress-strain curves from materials with varying ductility (e.g., olivine, Ti, W).
  • To assess the impact of machine stiffness on yield stress identification and the choice of analysis conventions.

Proposed method

  • Use three reference materials—fused silica, sapphire, and glassy carbon—with known elastic moduli and Poisson’s ratios to calibrate the system.
  • Perform elastic load-displacement measurements at low loads to avoid plasticity and ensure validity of Hertzian contact mechanics.
  • Parametrize the effective tip radius as a function of applied load using the measured harmonic contact stiffness and Hertzian contact theory.
  • Simultaneously calibrate the machine stiffness by fitting the measured stiffness data to the Hertzian model with adjustable machine compliance.
  • Apply the calibrated parameters to extract indentation stress-strain curves from materials with unknown moduli (olivine, Ti, W) using continuous stiffness measurement.
  • Test the influence of machine stiffness on yield stress identification and compare results across different conventions for pop-in and size effect analysis.
Figure 1: a) Load-displacement data collected with a spherical tip with a nominal radius of 10 μ m in different materials with known moduli. b) Difference between measured displacements in two materials at similar load. The end cut-off load for each set of experiments is marked by the dashed horizon
Figure 1: a) Load-displacement data collected with a spherical tip with a nominal radius of 10 μ m in different materials with known moduli. b) Difference between measured displacements in two materials at similar load. The end cut-off load for each set of experiments is marked by the dashed horizon

Experimental results

Research questions

  • RQ1How can the effective tip radius and machine stiffness be independently calibrated in spherical nanoindentation using only elastic reference materials?
  • RQ2To what extent does machine stiffness affect the accuracy of yield stress determination in spherical nanoindentation?
  • RQ3How does the choice of analysis convention influence the interpretation of indentation size effects and pop-in behavior?
  • RQ4Can a unified calibration workflow improve the consistency and reliability of indentation stress-strain curves across different materials and instruments?
  • RQ5What is the impact of tip shape deviations from perfect sphericity on stiffness and modulus measurements?

Key findings

  • The proposed calibration workflow enables independent and accurate determination of effective tip radius and machine stiffness using only elastic indentation data on three reference materials.
  • The effective tip radius was found to vary with load, and this dependence was successfully parametrized, improving accuracy over constant-radius assumptions.
  • Systematic variation in Young’s modulus with depth was observed and validated, confirming the reliability of the calibration approach.
  • The machine stiffness significantly influences the extracted yield stress, with differences of up to 15% observed depending on the calibration method.
  • The choice of convention for identifying yield stress and pop-in had a measurable impact on the reported indentation size effect, highlighting the need for standardized protocols.
  • The workflow was successfully applied to extract indentation stress-strain curves from olivine, titanium, and tungsten, demonstrating its utility across materials with varying ductility.
Figure 2: Summary of results for effective radius determined as the slope of a line fit through data calculated as the subtraction of elastic load-displacement curves at the same load in different reference materials following the method of Li et al. [ 2013 ] (Equation 8 ). The dashed line represent
Figure 2: Summary of results for effective radius determined as the slope of a line fit through data calculated as the subtraction of elastic load-displacement curves at the same load in different reference materials following the method of Li et al. [ 2013 ] (Equation 8 ). The dashed line represent

Read this paper

Open the full text in the Nubint reader and ask about any passage as you read.

Read this paper on Nubint

This review was generated by AI from the original paper. Please check the paper before citing it.